FLUGASCHE ENTHALTENDES ZEMENTMATERIAL

Rapid curing, high strength cementitious binder mixtures are provided containing fly ash and an alkali metal or alkaline earth metal silicate binder that has a weight ratio of SiO2:M2O of about 0.20:1 to about 0.75:1 wherein M is selected from the group consisting of Li, Na, K, +E,fra 1/2+EE Ca and...

Full description

Saved in:
Bibliographic Details
Main Authors SILVERSTRIM, THOMAS, SAMADI, ANAMOLAH, LARRALDE, JESUS, ROSTAMI, HOSSEIN
Format Patent
LanguageGerman
Published 15.05.2004
Edition7
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Rapid curing, high strength cementitious binder mixtures are provided containing fly ash and an alkali metal or alkaline earth metal silicate binder that has a weight ratio of SiO2:M2O of about 0.20:1 to about 0.75:1 wherein M is selected from the group consisting of Li, Na, K, +E,fra 1/2+EE Ca and +E,fra 1/2+EE Mg. The cementitious binder mixtures can be mixed with aggregates to provide mortar and concrete mixtures. Any of the binder, mortar and concrete mixtures can be cured under elevated temperatures to yield high strength products.
Bibliography:Application Number: AT19960905481T