WHISKERSVERSTÄRKTER KERAMISCHER KÖRPER

According to the present invention there is now provided a method of manufacturing a whisker reinforced ceramic body comprising 2-50 % by volume whiskers and/or fibers and/or platelets and/or submicron particles in a ceramic matrix by powder metallurgical methods, i.e., dispersion in a suitable liqu...

Full description

Saved in:
Bibliographic Details
Main Author COLLIN, MARIANNE
Format Patent
LanguageGerman
Published 15.03.2000
Edition7
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:According to the present invention there is now provided a method of manufacturing a whisker reinforced ceramic body comprising 2-50 % by volume whiskers and/or fibers and/or platelets and/or submicron particles in a ceramic matrix by powder metallurgical methods, i.e., dispersion in a suitable liquid, granulation, compaction and sintering. If the granulation is performed by freeze granulation a ceramic body with homogeneous structure with essentially no granule borders is obtained.
Bibliography:Application Number: AT19930850149T