EISENBASISLEGIERUNG ZUR VERWENDUNG BEI ERHÖHTER TEMPERATUR UND WERKZEUG AUS DIESER LEGIERUNG

The ferrous alloy contains (wt.%) 0.3-0.5 C; 0.4-1.6 Si; 0.3-0.8 Mn; 3.2-6.5 Cr; 0-2 Mo; 0-3 W; 0.95-2 (Mo + W/2); 0.25-1.2 V; 0.75-1.6 Al; 1.2-2.6 (Al + Si); 0-0.2 Nb; 0-0.15 Ti; max 0.35 Ni; max 0.015N; and balance Fe.

Saved in:
Bibliographic Details
Main Authors LENGER HUBERT, SCHWEIGER HERBERT
Format Patent
LanguageGerman
Published 15.03.1997
Edition6
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The ferrous alloy contains (wt.%) 0.3-0.5 C; 0.4-1.6 Si; 0.3-0.8 Mn; 3.2-6.5 Cr; 0-2 Mo; 0-3 W; 0.95-2 (Mo + W/2); 0.25-1.2 V; 0.75-1.6 Al; 1.2-2.6 (Al + Si); 0-0.2 Nb; 0-0.15 Ti; max 0.35 Ni; max 0.015N; and balance Fe.
Bibliography:Application Number: AT51695