Solution-combustion synthesis of Tb 3+-doped Y 3Al 5O 12 nanoparticles

Nano-sized YAG:Tb powder phosphors were prepared by a solution-combustion method, using the general inorganic salts as starting materials. The X-ray diffraction (XRD) measurements showed that the precursor can be well-crystallized at 900 °C. As-prepared particles have sizes mostly in the range betwe...

Full description

Saved in:
Bibliographic Details
Published inJournal of luminescence Vol. 129; no. 4; pp. 401 - 405
Main Authors Fadlalla, H.M.H., Tang, C.C., Elsanousi, A., Ding, X.X., Qi, S.R.
Format Journal Article
LanguageEnglish
Published Elsevier B.V 2009
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Nano-sized YAG:Tb powder phosphors were prepared by a solution-combustion method, using the general inorganic salts as starting materials. The X-ray diffraction (XRD) measurements showed that the precursor can be well-crystallized at 900 °C. As-prepared particles have sizes mostly in the range between 30 and 100 nm as obtained by scanning electron microscope (SEM) and transition electron microscope (TEM). Selected area electron diffraction (SAED) patterns proved that the larger particles are monocrystalline. The effects of annealing temperature and Tb-doping concentration on the luminescence intensity were studied.