Preparation and some properties of pulsed laser deposited YFeO 3 films

YFeO 3 orthoferrite films have been deposited on to quartz and sapphire substrates by pulsed laser deposition. The films crystallize when annealed at temperatures in the range 750 to 900°C. The perpendicular hysteresis loops are rectangular with a maximum coercivity of 9 kOe. The Faraday rotation at...

Full description

Saved in:
Bibliographic Details
Published inJournal of magnetism and magnetic materials Vol. 147; no. 3; pp. L221 - L224
Main Authors Krishnan, R., Lisfi, A., Guyot, M., Cagan, V.
Format Journal Article
LanguageEnglish
Published Elsevier B.V 1995
Online AccessGet full text

Cover

Loading…
More Information
Summary:YFeO 3 orthoferrite films have been deposited on to quartz and sapphire substrates by pulsed laser deposition. The films crystallize when annealed at temperatures in the range 750 to 900°C. The perpendicular hysteresis loops are rectangular with a maximum coercivity of 9 kOe. The Faraday rotation at 633 nm wavelength is in the range 4–5 × 10 3 deg/cm.