Thermal diffusivity/conductivity of AECL Li 2TiO 3 ceramic

The thermal diffusivity and heat capacity of lithium titanate (Li 2TiO 3), produced by AECL (Chalk River, ON, Canada), has been measured in the temperature range 300 to 1000 K, using the laser flash technique. From these data, the thermal conductivity has been calculated. The thermal conductivity ra...

Full description

Saved in:
Bibliographic Details
Published inJournal of nuclear materials Vol. 232; no. 1; pp. 65 - 68
Main Authors Davis, J.W., Haasz, A.A.
Format Journal Article
LanguageEnglish
Published Elsevier B.V 1996
Online AccessGet full text

Cover

Loading…
More Information
Summary:The thermal diffusivity and heat capacity of lithium titanate (Li 2TiO 3), produced by AECL (Chalk River, ON, Canada), has been measured in the temperature range 300 to 1000 K, using the laser flash technique. From these data, the thermal conductivity has been calculated. The thermal conductivity ranged in value from 3 W/mK at 300 K, decreasing to 2.2 W/mK in the 425 to 675 K temperature range, and then increasing to ∼ 2.6 W/mK at 1000 K.
ISSN:0022-3115
1873-4820
DOI:10.1016/0022-3115(96)00396-0