Effect of the milling time on the magnetic properties of powder compositions of the Sm2Fe17Nx intermetallic compound and an Nd–Fe–B alloy

The effect of the wet milling time on the magnetic properties of powder compositions consisting of the hard magnetic Sm 2 Fe 17 N x ( x = 2.9–3.0) nitride and a rapidly quenched Nd 9.6 Fe 76.3 Co 4.3 Zr 3.4 B 6.4 (at %) alloy, which are taken in different mass proportions, is studied. The compositio...

Full description

Saved in:
Bibliographic Details
Published inRussian metallurgy Metally Vol. 2017; no. 10; pp. 807 - 812
Main Authors Savchenko, A. G., Menushenkov, V. P., Plastinin, A. Yu, Shchetinin, I. V., Bordyuzhin, I. G., Ryazantsev, V. A., Verbetskii, V. N., Movlaev, E. A.
Format Journal Article
LanguageEnglish
Published Moscow Pleiades Publishing 01.10.2017
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The effect of the wet milling time on the magnetic properties of powder compositions consisting of the hard magnetic Sm 2 Fe 17 N x ( x = 2.9–3.0) nitride and a rapidly quenched Nd 9.6 Fe 76.3 Co 4.3 Zr 3.4 B 6.4 (at %) alloy, which are taken in different mass proportions, is studied. The compositions containing no more than 20 wt % alloy are found to exhibit a substantial increase in the magnetic characteristics as compared to those of the nitride. It is shown that the determining effect on the coercivity is related to the degree of structural imperfection of Nd–Fe–B powders, whereas the specific remanent magnetization and the specific magnetization in a field of 2 T are determined by the corresponding characteristics of the alloy. The optimum composition and efficient treatment conditions for powder mixtures are determined.
ISSN:0036-0295
1555-6255
DOI:10.1134/S0036029517100202