무전해 Ni-Zn-P 도금의 속도 및 안정성에 미치는 첨가제의 영향

The effect of additives such as complexing agents, stabilzers and boric acid on the bath stability and the deposition rate of electroless black Ni-Zn plating has been examined. The deposits obtained became black and showed an amorphous structure. The significant increasing in the deposition rate was...

Full description

Saved in:
Bibliographic Details
Published inBiuletyn Uniejowski Vol. 36; no. 4; pp. 317 - 323
Main Authors 오영주(Young-Joo Oh), 황경진(Kyoung-Jin Hwang), 정원용(WonYoung Jeung), 이만승(Man-Seung Lee)
Format Journal Article
LanguageKorean
Published 한국표면공학회 2003
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The effect of additives such as complexing agents, stabilzers and boric acid on the bath stability and the deposition rate of electroless black Ni-Zn plating has been examined. The deposits obtained became black and showed an amorphous structure. The significant increasing in the deposition rate was not found when only glycine and citric acid were used as complexing agents. The deposition rate increased up to 3 and 4 times by adding malic acid and glycolic acid as an additional complexing agent, respectively. The stabilizers and the boric acid, however, had little influence on the deposition rate.
Bibliography:KISTI1.1003/JNL.JAKO200311921890670
ISSN:1225-8024
2299-8403