저온 풀림 처리 Alloy 600이 1차수 응력 부식 균열에 가장 예민한 이유
It has been proposed that a primary water stress corrosion cracking (PWSCC) in pressurized water reactor (PWR) is governed by a lattice contraction due to a short range ordering reaction in Alloy 600. This leads researcher to think that the kinetics of lattice contraction may control a susceptibilit...
Saved in:
Published in | 대한금속·재료학회지, 58(12) Vol. 58; no. 12; pp. 815 - 821 |
---|---|
Main Authors | , , , , , |
Format | Journal Article |
Language | Korean |
Published |
대한금속재료학회
05.12.2020
대한금속·재료학회 |
Subjects | |
Online Access | Get full text |
ISSN | 1738-8228 2288-8241 |
Cover
Summary: | It has been proposed that a primary water stress corrosion cracking (PWSCC) in pressurized water reactor (PWR) is governed by a lattice contraction due to a short range ordering reaction in Alloy 600. This leads researcher to think that the kinetics of lattice contraction may control a susceptibility of PWSCC in Alloy 600. A lattice variation with ordering treatment at 400 ℃ was systematically investigated using high resolution neutron diffraction(HRPD) in high temperature mill anneal (HTMA), low temperature mill anneal (LTMA), and sensitized (SEN) Alloy 600. The results showed that ordering treatment caused an isotropic lattice contraction due to short range ordering (SRO) reaction. The lattice contractions of (111) plane are saturated to be 0.04% in 4 to 1500 hours at 400 ℃ according to prior treatment condition. The lattice contraction in the magnitude of 0.03% of (111) plane in LTMA Alloy 600 is faster by 8 times and 66 times than that of SEN and HTMA, respectively. This fact may explain why the LTMA is most susceptible to PWSCC through of kinetics of lattice contraction in Alloy 600. Thus, it is possible to conclude that the susceptibility of Alloy 600 to PWSCC is governed by the kinetics of (111) lattice contraction.
(Received August 11, 2020; Accepted October 7, 2020) |
---|---|
Bibliography: | The Korean Institute of Metals and Materials |