물분해용 Fe2O3/Na2Ti6O13/FTO 박막 제조 및 특성평가

One dimensional (1D) Na2Ti6OIi nanorods with 70 nm in diameter was synthesized by a molten salt method. Using the synthesized nanorods, about 750 nm thick Na2TisO,3 film was coated on Fluorine-doped till oxide (FTO) glasss substrate by the Layer-by-layer self-assembly(LBL-SA) method in which a repet...

Full description

Saved in:
Bibliographic Details
Published inCorrosion science and technology Vol. 11; no. 2; pp. 65 - 69
Main Authors 윤강섭, Kang Seop Yun, 구혜경, Hye Kyung Ku, 강우승, Woo Seung Kang, 김선재, Sun Jae Kim
Format Journal Article
LanguageKorean
Published 한국부식방식학회 30.04.2012
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:One dimensional (1D) Na2Ti6OIi nanorods with 70 nm in diameter was synthesized by a molten salt method. Using the synthesized nanorods, about 750 nm thick Na2TisO,3 film was coated on Fluorine-doped till oxide (FTO) glasss substrate by the Layer-by-layer self-assembly(LBL-SA) method in which a repetitive self-assembling of ions containing an opposite electric charge in an aqueous solution was utilized. Using the Kubelka-Munk function, the band gap energy of the ID-Na2Ti6O13 nanorods was nalyzed to be 3.5eV. On the other hand, the band gap energy of the Na2Ti6O13 film coated on FTC) was found to be a reduced value of 2.9eV, resulting from the nano-scale and high porosity of the film processed by LBL-SA method, which was favorable for the photo absorption capability, A significant improvement of photocurrent and onset voltage was observed with the Na2Ti6O13 film incorporated into the conventional Fe203 photoelectrode: the photocurrent increased from 0.25 to 0.82 mA/cm2, the onset voltage decreased from 0.95 to 0.78 V.