酸化鉄の還元がハイパーコールを配合したフェロコークスの強度に及ぼす影響

This study investigates the dominant factors affecting the strength of ferro-coke, which is produced by blending iron oxide with coal particles, with the addition of hyper-coal (HPC), to produce a high reactivity and strong coke. A diametral compression test for ferro-coke with and without HPC addit...

Full description

Saved in:
Bibliographic Details
Published in鉄と鋼 Vol. 105; no. 10; pp. 957 - 964
Main Authors 齋藤, 泰洋, 松下, 洋介, 松尾, 翔平, 内田, 中, 山崎, 義昭, 青木, 秀之, 濱口, 眞基
Format Journal Article
LanguageJapanese
Published 一般社団法人 日本鉄鋼協会 2019
Subjects
Online AccessGet full text
ISSN0021-1575
1883-2954
DOI10.2355/tetsutohagane.TETSU-2019-046

Cover

More Information
Summary:This study investigates the dominant factors affecting the strength of ferro-coke, which is produced by blending iron oxide with coal particles, with the addition of hyper-coal (HPC), to produce a high reactivity and strong coke. A diametral compression test for ferro-coke with and without HPC addition is performed. A three-dimensional ferro-coke model is then developed using micro X-ray computed tomography, and the relative proportions of pore, pore wall, iron, and pore space surrounding the iron particles, termed here “defect”, are quantified using this model. Moreover, a stress analysis is performed for the ferro-coke model. The diametral compression tests indicate that the strength of ferro-coke increases with the increasing blending ratio of HPC. The image-based modeling indicates that the wall thickness increases and stress concentration is relaxed with increasing addition of HPC due to enhancement of the adhesiveness of coal particles. On the other hand, the relative proportion of the “defect” is independent of HPC addition. Therefore, ferro-coke strength is found to be determined not by the “defect” around iron oxide but by the wall thickness.