Tensile shear strength of laser welded Ti-6Al-4V lap joints

Tensile shearing tests are used to investigate the mechanical property of laser welded Ti-6Al-4V lap joints. The load per length of weld bead is introduced to evaluate the bearing ability of laser lap joints, and the failure load ranges from 394 to 502N/mm. The optima parameters for 0.8mm thick Ti-6...

Full description

Saved in:
Bibliographic Details
Published in2011 Second International Conference on Mechanic Automation and Control Engineering pp. 741 - 744
Main Authors Donghai Cheng, Yiping Chen, Dean Hu, Yeping Zhou
Format Conference Proceeding
LanguageEnglish
Published IEEE 01.07.2011
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Tensile shearing tests are used to investigate the mechanical property of laser welded Ti-6Al-4V lap joints. The load per length of weld bead is introduced to evaluate the bearing ability of laser lap joints, and the failure load ranges from 394 to 502N/mm. The optima parameters for 0.8mm thick Ti-6Al-4V alloy is 1800~2350W laser power and 1.5~2.5m/min welding velocity.