Dynamic dissolution of CO2/H2O(g)-gasified coke by slag containing FeO

In top gas recycling-oxygen blast furnace (TGR-BF) and injection coke oven gas-blast furnace (COG-BF), lower coke ratio highlight the importance of coke in the melting and dropping zone. To understand the deterioration of coke in lower blast furnace, the dynamic dissolution of CO 2 /H 2 O-gasified c...

Full description

Saved in:
Bibliographic Details
Published inIronmaking & steelmaking Vol. 45; no. 9; pp. 821 - 827
Main Authors Liu, Yingli, Xue, Qingguo, Wang, Guang, Wang, Jingsong
Format Journal Article
LanguageEnglish
Published London, England Taylor & Francis 21.10.2018
SAGE Publications
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:In top gas recycling-oxygen blast furnace (TGR-BF) and injection coke oven gas-blast furnace (COG-BF), lower coke ratio highlight the importance of coke in the melting and dropping zone. To understand the deterioration of coke in lower blast furnace, the dynamic dissolution of CO 2 /H 2 O-gasified coke by slag containing FeO and reaction kinetics were analysed. The results showed that the coke deterioration was more serious in CO 2 than in H 2 O for the same gasification ratio. To understand the internal variation of coke, pore distribution and microstructure of coke were observed using mercury porosimeter and scanning electron microscope (SEM). For the same gasification ratio, pore structure was more uniform in H 2 O than in CO 2 . In addition, the kinetics of coke's reaction with FeO in slag was analysed.