The effect of synthesis time to particle size of Bi4Ti3O12 which synthesized using molten single salt NaCl method
Bi4Ti3O12 was synthesized by the molten salt method using single salt NaCl with calcination time variations: 2, 4, 8, and 16 hours at 900 °C. The effect of time synthesis on particle size and morphology was investigated. The X-ray diffraction data showed that the sample Bi4Ti3O12 was successfully sy...
Saved in:
Published in | IOP conference series. Earth and environmental science Vol. 456; no. 1 |
---|---|
Main Authors | , , , |
Format | Journal Article |
Language | English |
Published |
Bristol
IOP Publishing
01.02.2020
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | Bi4Ti3O12 was synthesized by the molten salt method using single salt NaCl with calcination time variations: 2, 4, 8, and 16 hours at 900 °C. The effect of time synthesis on particle size and morphology was investigated. The X-ray diffraction data showed that the sample Bi4Ti3O12 was successfully synthesis and there is not found any impurities. The image from scanning electron microscopy showed that the shape of Bi4Ti3O12 particle is plate-like and particle size increases as calcination time. |
---|---|