Corrosion resistance of Ti–6Al–4V alloy with nitride coatings in Ringer’s solution

► Nitride coatings were formed on Ti–6Al–4V alloy by thermodiffusion saturation. ► Nitrides improve corrosion resistance of alloy in Ringer’s solution at 36 and 40°С. ► Corrosion resistance increases with increase of TiN phase in nitride coating. ► Corrosion resistance is determined significantly by...

Full description

Saved in:
Bibliographic Details
Published inCorrosion science Vol. 66; pp. 392 - 398
Main Authors Pohrelyuk, I.M., Fedirko, V.M., Tkachuk, O.V., Proskurnyak, R.V.
Format Journal Article
LanguageEnglish
Published Kidlington Elsevier Ltd 01.01.2013
Elsevier
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:► Nitride coatings were formed on Ti–6Al–4V alloy by thermodiffusion saturation. ► Nitrides improve corrosion resistance of alloy in Ringer’s solution at 36 and 40°С. ► Corrosion resistance increases with increase of TiN phase in nitride coating. ► Corrosion resistance is determined significantly by quality of nitride coating. The corrosion behaviour of Ti–6Al–4V alloy with nitride coatings was investigated in Ringer’s solution at 36 and 40°С. Nitride coatings of different composition, thickness and surface quality were formed because of changing nitrogen partial pressure from 1 to 105Ра and nitriding temperature from 850 to 900°С. Results shown that nitride coatings improve anticorrosion properties of alloy at both solution temperatures. Corrosion resistance of alloy increases with the content increase of TiN phase in nitride coating. With increase of temperature from 36 to 40°С the corrosion resistance of alloy is determined significantly by quality of nitride coating.
Bibliography:ObjectType-Article-1
SourceType-Scholarly Journals-1
ObjectType-Feature-2
content type line 23
ISSN:0010-938X
1879-0496
DOI:10.1016/j.corsci.2012.10.005