In Vivo and In Vitro Degradation Behavior of Magnesium Alloys as Biomaterials

The corrosion behavior of pure Mg,AZ31,and AZ91D were evaluated in various in vitro and in vivo environments to investigate the potential application of these metals as biodegradable implant materials.DC polarization tests and immersion tests were performed in different simulated body solutions,such...

Full description

Saved in:
Bibliographic Details
Published inJournal of materials science & technology Vol. 28; no. 3; pp. 261 - 267
Main Authors Xue, Dingchuan, Yun, Yeoheung, Tan, Zongqing, Dong, Zhongyun, Schulz, Mark J.
Format Journal Article
LanguageEnglish
Published Elsevier Ltd 01.03.2012
Subjects
Online AccessGet full text
ISSN1005-0302
1941-1162
DOI10.1016/S1005-0302(12)60051-6

Cover

Loading…
More Information
Summary:The corrosion behavior of pure Mg,AZ31,and AZ91D were evaluated in various in vitro and in vivo environments to investigate the potential application of these metals as biodegradable implant materials.DC polarization tests and immersion tests were performed in different simulated body solutions,such as distilled(DI) water,simulated body fluid(SBF) and phosphate buffered solution(PBS).Mg/Mg alloys were also implanted in different places in a mouse for in vivo weight loss and biocompatibility investigations.The in vivo subcutis bio-corrosion rate was lower than the corrosion rate for all of the in vitro simulated corrosive environments.The Mg/Mg alloys were biocompatible based on histology results for the liver,heart,kidney,skin and lung of the mouse during the two months implantation.Optical microscopy and scanning electron microscopy were carried out to investigate the morphology and topography of Mg/Mg alloys after immersion testing and implantation to understand the corrosion mechanisms.
Bibliography:21-1315/TG
The corrosion behavior of pure Mg,AZ31,and AZ91D were evaluated in various in vitro and in vivo environments to investigate the potential application of these metals as biodegradable implant materials.DC polarization tests and immersion tests were performed in different simulated body solutions,such as distilled(DI) water,simulated body fluid(SBF) and phosphate buffered solution(PBS).Mg/Mg alloys were also implanted in different places in a mouse for in vivo weight loss and biocompatibility investigations.The in vivo subcutis bio-corrosion rate was lower than the corrosion rate for all of the in vitro simulated corrosive environments.The Mg/Mg alloys were biocompatible based on histology results for the liver,heart,kidney,skin and lung of the mouse during the two months implantation.Optical microscopy and scanning electron microscopy were carried out to investigate the morphology and topography of Mg/Mg alloys after immersion testing and implantation to understand the corrosion mechanisms.
Mg/Mg alloys In vitro/in vivo testing Bio-degradation rate Biocompatibility
ObjectType-Article-2
SourceType-Scholarly Journals-1
ObjectType-Feature-1
content type line 23
ISSN:1005-0302
1941-1162
DOI:10.1016/S1005-0302(12)60051-6