Assessment of creeping discharge initiated by metal particles on the silicone rubber/XLPE interface in cable joints

Creeping breakdown caused by metal particles on the silicone rubber/XLPE interface of prefabricated cable joints often happens. Study on the development process of such insulation defect-led partial discharge (PD) can serve as a basis for the assessment of its severity level. In this paper, metal pa...

Full description

Saved in:
Bibliographic Details
Published inJournal of Electrical Engineering Vol. 70; no. 5; pp. 370 - 378
Main Authors Chang, Wen-Zhi, Du, Fei, Bi, Jian-Gang, Yuan, Shuai, Gong, Yan-Peng, Yang, Yuan
Format Journal Article
LanguageEnglish
Published Bratislava Sciendo 01.09.2019
De Gruyter Poland
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Creeping breakdown caused by metal particles on the silicone rubber/XLPE interface of prefabricated cable joints often happens. Study on the development process of such insulation defect-led partial discharge (PD) can serve as a basis for the assessment of its severity level. In this paper, metal particles are sandwiched on the rubber/XLPE interface of a 35 kV prefabricated cable joint to simulate a creeping defect.