High temperature deformation characteristics of Zirlo™ tubing via ring-creep and burst tests

Fuel cladding tubing acting as a barrier between coolant and radioactive fuel pellets in light water reactors undergo a combination of mechanical and thermal effects along with corrosive conditions during normal operations as well as accident situations, such as LOCA, etc. Therefore, the mechanical...

Full description

Saved in:
Bibliographic Details
Published inNuclear engineering and design Vol. 241; no. 3; pp. 599 - 602
Main Authors Seok, C.S., Marple, B., Song, Y.J., Gollapudi, S., Charit, I., Murty, K.L.
Format Journal Article
LanguageEnglish
Published Elsevier B.V 01.03.2011
Online AccessGet full text

Cover

Loading…
More Information
Summary:Fuel cladding tubing acting as a barrier between coolant and radioactive fuel pellets in light water reactors undergo a combination of mechanical and thermal effects along with corrosive conditions during normal operations as well as accident situations, such as LOCA, etc. Therefore, the mechanical integrity of the cladding tubing is of critical importance. In this study, high temperature deformation characteristics of niobium-containing zirconium alloy cladding materials (Zirlo™) have been evaluated via both ring-creep and burst tests. Creep-rupture data are presented in terms of Larson–Miller parameters (LMP). Data (creep rate vs. stress) from ring-creep and burst tests are analyzed, and operating deformation mechanisms are elucidated. This study demonstrates that the hoop creep data obtained from ring-creep and burst tests are equivalent, and one can be replaced with the other, if needed, in order to evaluate creep life.