Halogen effect for improving high temperature oxidation resistance of Ti-50Al by anodization
[Display omitted] •Anodization can improve the high temperature oxidation resistance of Ti-50Al.•The improved high temperature oxidation resistance is the result of halogen effect.•Anodized Ti-50Al with holes and micro-cracks will be self-repaired during oxidation.•The oxide scale with two layer str...
Saved in:
Published in | Applied surface science Vol. 407; pp. 246 - 254 |
---|---|
Main Authors | , , , , |
Format | Journal Article |
Language | English |
Published |
Elsevier B.V
15.06.2017
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | [Display omitted]
•Anodization can improve the high temperature oxidation resistance of Ti-50Al.•The improved high temperature oxidation resistance is the result of halogen effect.•Anodized Ti-50Al with holes and micro-cracks will be self-repaired during oxidation.•The oxide scale with two layer structures is formed gradually during oxidation.
The high temperature oxidation resistance of Ti-50Al was significantly improved via halogen effect which was achieved by anodizing in an ethylene glycol solution containing with fluorine ion. The anodized Ti-50Al with holes and micro-cracks could be self-repaired during oxidation at 1000°C. The thickness of the oxide scale increases with the prolonging of oxidation time. On the basis of halogen effect for improving the high temperature oxidation resistance of Ti-50Al by anodization, only fluorine addition into the electrolyte can effectively improve the high temperature oxidation resistance of Ti-50Al. |
---|---|