Implementation of long-wavelength cut-off filters based on critical angle

Our first attempts at the fabrication of long-wavelength infrared cut-off filters with extended transmission and rejection regions that are based on the use of the critical angle, the dispersion of refractive indices, and on thin-film interference were not very successful. The design of the filter c...

Full description

Saved in:
Bibliographic Details
Published inApplied optics. Optical technology and biomedical optics Vol. 50; no. 9; p. C396
Main Authors Guo, Yanen, Dobrowolski, J A, Li, Li, Poitras, Daniel, Tiwald, Tom
Format Journal Article
LanguageEnglish
Published United States 20.03.2011
Online AccessGet more information

Cover

Loading…
More Information
Summary:Our first attempts at the fabrication of long-wavelength infrared cut-off filters with extended transmission and rejection regions that are based on the use of the critical angle, the dispersion of refractive indices, and on thin-film interference were not very successful. The design of the filter consisted of layers placed at the interface between two high-index prisms. Using the available deposition equipment, the layers produced were porous and very rough. The pores adsorbed water vapor, which resulted in absorption. The roughness made the process of optical contacting very difficult. In this paper we describe the adjustments in the design and deposition processes that allowed us to obtain filters with a better and more stable performance.