Different effect of NiMnCo or FeNiCo on the growth of type-Ⅱa large diamonds with Ti/Cu as nitrogen getter

In order to synthesize high-quality type-Ⅱa large diamond, the selection of catalyst is very important, in addition to the nitrogen getter. In this paper, type-IIa large diamonds are grown under high pressure and high temperature(HPHT) by using the temperature gradient method(TGM), with adopting Ti/...

Full description

Saved in:
Bibliographic Details
Published inChinese physics B Vol. 26; no. 6; pp. 454 - 458
Main Author 李尚升 张贺 宿太超 胡强 胡美华 龚春生 马红安 贾晓鹏 李勇 肖宏宇
Format Journal Article
LanguageEnglish
Published 01.06.2017
Online AccessGet full text

Cover

Loading…
More Information
Summary:In order to synthesize high-quality type-Ⅱa large diamond, the selection of catalyst is very important, in addition to the nitrogen getter. In this paper, type-IIa large diamonds are grown under high pressure and high temperature(HPHT) by using the temperature gradient method(TGM), with adopting Ti/Cu as the nitrogen getter in Ni70Mn25Co5(abbreviated as NiMnCo) or Fe(55)Ni(29)Co(16)(abbreviated FeNiCo) catalyst. The values of nitrogen concentration(Nc) in both synthesized high-quality diamonds are less than 1 ppm, when Ti/Cu(1.6 wt%) is added in the FeNiCo or Ti/Cu(1.8 wt%) is added in the NiMnCo. The difference in solubility of nitrogen between both catalysts at HPHT is the basic reason for the different effect of Ti/Cu on eliminating nitrogen. The nitrogen-removal efficiency of Ti/Cu in the NiMnCo catalyst is less than in the FeNiCo catalyst. Additionally, a high-quality type-Ⅱa large diamond size of 5.0 mm is obtained by reducing the growth rate and keeping the nitrogen concentration of the diamond to be less than 1 ppm, when Ti/Cu(1.6 wt%) is added in the FeNiCo catalyst.
Bibliography:high pressure and high temperature, catalyst, nitrogen getter, type-Ⅱa large diamond
In order to synthesize high-quality type-Ⅱa large diamond, the selection of catalyst is very important, in addition to the nitrogen getter. In this paper, type-IIa large diamonds are grown under high pressure and high temperature(HPHT) by using the temperature gradient method(TGM), with adopting Ti/Cu as the nitrogen getter in Ni70Mn25Co5(abbreviated as NiMnCo) or Fe(55)Ni(29)Co(16)(abbreviated FeNiCo) catalyst. The values of nitrogen concentration(Nc) in both synthesized high-quality diamonds are less than 1 ppm, when Ti/Cu(1.6 wt%) is added in the FeNiCo or Ti/Cu(1.8 wt%) is added in the NiMnCo. The difference in solubility of nitrogen between both catalysts at HPHT is the basic reason for the different effect of Ti/Cu on eliminating nitrogen. The nitrogen-removal efficiency of Ti/Cu in the NiMnCo catalyst is less than in the FeNiCo catalyst. Additionally, a high-quality type-Ⅱa large diamond size of 5.0 mm is obtained by reducing the growth rate and keeping the nitrogen concentration of the diamond to be less than 1 ppm, when Ti/Cu(1.6 wt%) is added in the FeNiCo catalyst.
Shang-Sheng Li1, He Zhang1, Tai-Chao Su1, Qiang Hu1 Mei-Hua Hu1, Chun-Sheng Gong1, Hon-An Ma2, Xiao-Peng Jia2, Yong Li3, Hong-Yu Xiao4 ( 1 School of Materials Science and Engineering, Henan Polytechnic University, Jiaozuo 454000, China ; 2 State Key Laboratory of Superhard Materials, Jilin University, Changchun 130012, China; 3 School of Data Science, Tongren University, Tongren 554300, China ;4Department of Mathematics and Physics, Luoyang Institute of Science and Technology, Luoyang 471023, China)