Implication of operation time on low-temperature catalytic oxidation of chloroaromatic organics over VOx/TiO2 catalysts: Deactivation mechanism analysis

Three commercial granular catalysts were collected according to their operation time (fresh, two years, and three years, denoted as Cata-1, Cata-2, and Cata-3, respectively). The catalytic efficiency and CO2/CO/HCl selectivity of 1,2-dichlorobenzene (1,2-DCB) catalytic oxidation were investigated at...

Full description

Saved in:
Bibliographic Details
Published inJournal of cleaner production Vol. 372; p. 133477
Main Authors Ma, Yunfeng, Lai, Jianwen, Lin, Xiaoqing, Zhang, Hao, Du, Hailiang, Long, Jisheng, Yan, Jianhua, Li, Xiaodong
Format Journal Article
LanguageEnglish
Published Elsevier Ltd 20.10.2022
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Three commercial granular catalysts were collected according to their operation time (fresh, two years, and three years, denoted as Cata-1, Cata-2, and Cata-3, respectively). The catalytic efficiency and CO2/CO/HCl selectivity of 1,2-dichlorobenzene (1,2-DCB) catalytic oxidation were investigated at low temperature (150–200 °C). The Cata-1 showed excellent catalytic activities with high conversion efficiency (CE, 76.12–85.94%), CO2/CO selectivity (77.56–82.47%), and HCl selectivity (63.74–72.54%). The irreversible deactivation distinctly reduced the catalytic activities of Cata-2 and Cata-3, caused the decrease of catalytic reaction rate (k) and increase of apparent activation energy (Ea) from Cata-1 (1.59–2.18 s−1, 11.01 kJ/mol) to Cata-2 (0.12–0.38 s−1, 34.44 kJ/mol) and Cata-3 (0.007–0.125 s−1, 92.70 kJ/mol), respectively. Based on the abundant characteristic results and their correlation coefficient (R2) with 1/Ea, the S-poisoning was assigned as the major deactivation factor, while the implication factors also included alkali metals, heavy metals, HCl, fly ash, and the deposition substances formed with them. The deactivation pathways contained destroying surface porous structures and Brønsted acid sites, inhibiting the redox cycle of VOx, competing for surface reactive oxygen species, and blocking surface active sites. Based on these, two improvement suggestions were proposed to (1) develop new catalysts by reducing VOx content and introducing a second active component (eg., WOx, MoOx, CeOx, etc.); (2) develop new reactivated technologies. The former can impair the S-poisoning and improve the resistance for other implication factors and the redox ability of catalyst, and the latter was aim to sweep foreign residues, restore, or introduce surface reactive oxygen and available acid sites. The results provided essential basics for further improvement of granular catalyst and benefited the synergistic emission control of chloroaromatic organics and NOx from MSWI. [Display omitted] •The excellent low-temperature redox ability of fresh catalyst was investigated.•Long-term operation significantly decreased the catalytic activities of catalysts.•S-poisoning and foreign substances deposition were the major implication factors.•Deactivation pathways were revealed by abundant characteristic and statistical methods.•New catalysts and reactivated technologies were suggested to overcome deactivation effect.
ISSN:0959-6526
1879-1786
DOI:10.1016/j.jclepro.2022.133477