Sulfonated poly(ether ether ketone)/poly(amide imide) polymer blends for proton conducting membrane

Poly(amide imide) (PAI) was synthesized using 1,2,4-benzenetricarboxylic anhydride (BTBA) and 4,4′-methylenebis(phenyl isocyanate) (MBPI). SPEEK/PAI blend membranes were prepared and investigated by NMR, GPC, FT-IR and AFM. The chemical structures of PAI and SPEEK were characterized by using NMR and...

Full description

Saved in:
Bibliographic Details
Published inJournal of membrane science Vol. 280; no. 1; pp. 501 - 508
Main Authors Wu, Han-Lang, Ma, Chen-Chi M., Li, Chia-Hsun, Lee, Tzong-Ming, Chen, Chih-Yuan, Chiang, Chin-Lung, Wu, Chen
Format Journal Article
LanguageEnglish
Published Elsevier B.V 01.09.2006
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Poly(amide imide) (PAI) was synthesized using 1,2,4-benzenetricarboxylic anhydride (BTBA) and 4,4′-methylenebis(phenyl isocyanate) (MBPI). SPEEK/PAI blend membranes were prepared and investigated by NMR, GPC, FT-IR and AFM. The chemical structures of PAI and SPEEK were characterized by using NMR and FT-IR. The adsorption of the SPEEK/PAI blend membrane of water or methanol solution was also characterized. The significant swelling of the blend membrane in concentrated methanol solution was explained by the solubility parameter. The water diffusion coefficient ( D H 2 O ) was related to the lambda value of the membrane. The SPEEK/PAI blend membrane had a lower proton conductivity and methanol permeability than Nafion. However, the relative selectivity (proton conductivity divided by methanol permeability) of the SPEEK/PAI 70/30 (w/w) blend membrane was 3.46 × 10 4 S s cm −3, which is closed to that of Nafion (3.30 S s cm −3).