Effects of Liquid Contaminants on Heat Seal Strength of low-density polyethylene Film

Heat sealing is commonly applied for making form‐fill‐seal packages fabricated from thermoplastic films. One of the challenges frequently faced by the industry is inadvertent contamination of film–film interface by the product during filling, which can compromise package seal strength. In this study...

Full description

Saved in:
Bibliographic Details
Published inPackaging technology & science Vol. 25; no. 5; pp. 271 - 284
Main Authors Mihindukulasuriya, S., Lim, L.-T.
Format Journal Article
LanguageEnglish
Published Blackwell Publishing Ltd 01.08.2012
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Heat sealing is commonly applied for making form‐fill‐seal packages fabricated from thermoplastic films. One of the challenges frequently faced by the industry is inadvertent contamination of film–film interface by the product during filling, which can compromise package seal strength. In this study, the effects of dwell time (0.5–1.5 s), jaw pressure (28–1860 kPa), jaw configuration (narrow versus wide contact area) and jaw temperature (150°C–180°C) on the interface temperature and seal strength of a linear low‐density polyethylene (LLDPE) film were investigated. Three different film–film interface conditions were studied: (1) no contaminant; (2) with water contaminant; and (3) with vegetable oil contaminant. In the presence of liquid contaminant, jaw pressure played an important role in displacing the liquid from the seal area to form intact seals. Short dwell time (0.3 s) and low jaw temperature (150°C) was not favourable for forming intact seals in both water‐contaminated and vegetable oil‐contaminated films. The optimum jaw temperature and dwell time required to produce intact seals for oil contaminated films was 180°C and 0.3 s, respectively, whereas a combination of 165°C jaw temperature and 1 s dwell time was required to form intact seals for water‐contaminated films. Within the experimental conditions investigated, interface temperatures of 130°C–140°C resulted in the most optimum seal strength for both water‐contaminated and clean film specimens. Above 140°C, a weakening of seal strength was observed, presumably because of the change in melt flow characteristics and possible initiation of thermal degradation of the polymer. Copyright © 2011 John Wiley & Sons, Ltd. The presence of liquid contaminant(s) during the heat sealing of thermoplastic films can interfere with the formation of a robust seal. In this study, the effects of heat sealing process variables (dwell time, pressure, jaw configuration and temperature) on the interface temperature and seal strength characteristics of linear low‐density polyethylene (LLDPE) film were investigated under different film–film interface conditions. This study showed that the contaminant layer interacted strongly with sealing parameters and affected the seal strength characteristics significantly.