Calculation of the basic kinetic parameters of thermo-oxidative degradation of polyethylene and its copper-containing composites

Calculation of the basic kinetic parameters of thermo-oxidative destruction of initial, porous HDPE and copper-containing composites based on porous HDPE was carried out by the IKP method. It was shown that thermo-oxidation of these materials consisted of three stages: (1) the migration of oxygen mo...

Full description

Saved in:
Bibliographic Details
Published inPolymer degradation and stability Vol. 74; no. 2; pp. 291 - 295
Main Authors Trofimchuk, E.S, Yablokova, M.Y
Format Journal Article
LanguageEnglish
Published Oxford Elsevier Ltd 2001
Elsevier Science
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Calculation of the basic kinetic parameters of thermo-oxidative destruction of initial, porous HDPE and copper-containing composites based on porous HDPE was carried out by the IKP method. It was shown that thermo-oxidation of these materials consisted of three stages: (1) the migration of oxygen molecules to the active oxidising centres and the beginning of chain oxidation; (2) destruction of polymer molecules; and (3) thermodegradation of “nuclei”. However, porous HDPE was oxidised at lower temperature. Thermooxidation of copper-containing porous HDPE composite was characterised by the higher activation energy.