Quantitative Study on Abrasive Belt Wear Based on Geometric Parameters
In this paper, based on micro wear form, an approach that using protrusion height, average tool angle, blunt area ratio and coated density to describe the wear of abrasive belt is put forward. The method for calculating the above parameters are also introduced. In experiments, we use the profilomete...
Saved in:
Published in | Key engineering materials Vol. 764; pp. 156 - 163 |
---|---|
Main Authors | , , , |
Format | Journal Article |
Language | English |
Published |
Zurich
Trans Tech Publications Ltd
01.02.2018
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | In this paper, based on micro wear form, an approach that using protrusion height, average tool angle, blunt area ratio and coated density to describe the wear of abrasive belt is put forward. The method for calculating the above parameters are also introduced. In experiments, we use the profilometer to collect the abrasive belt surface data and draw figures of the above parameters under service time, which indicates that using topography parameters can describe the degree of belt wear. According to parameters changing slope, the abrasive belt service time is roughly divided into two stages, initial wear stage and stable wear stage but no abrupt wear stage. Initial worn stage grains suffer more stress, patterns of wear are mainly severe wear and pull-off, while stable wear stage grains bear less stress and pattern of worn is dominated by mild wear. In addition to that, the other parameters changing trend is agreed and synchronous with protrusion height. |
---|---|
Bibliography: | Special topic volume with invited peer reviewed papers only |
ISSN: | 1013-9826 1662-9795 1662-9795 |
DOI: | 10.4028/www.scientific.net/KEM.764.156 |