Collapse in Crystalline Structure and Decline in Catalytic Activity of Pt Nanoparticles on Reducing Particle Size to 1 nm

Combined experimental and computational studies show that, upon reducing the diameter of Pt nanoparticles down to 1 nm, a collapse in the crystalline structure occurs spontaneously and the thus-induced quantum size effect causes a decline in the catalytic activity toward hydrogen oxidation reaction...

Full description

Saved in:
Bibliographic Details
Published inJournal of the American Chemical Society Vol. 129; no. 50; pp. 15465 - 15467
Main Authors Sun, Yubao, Zhuang, Lin, Lu, Juntao, Hong, Xinlin, Liu, Peifang
Format Journal Article
LanguageEnglish
Published United States American Chemical Society 19.12.2007
Online AccessGet full text

Cover

Loading…
More Information
Summary:Combined experimental and computational studies show that, upon reducing the diameter of Pt nanoparticles down to 1 nm, a collapse in the crystalline structure occurs spontaneously and the thus-induced quantum size effect causes a decline in the catalytic activity toward hydrogen oxidation reaction (HOR). The conversion from crystalline to amorphous structure is rationalized by molecular dynamic simulations; and the special electronic structure of amorphous Pt nanoparticles is revealed via density functional calculations. Not only has the present work estimated the Pt utilization limit for HOR, but it also expands the structure−activity relationship of Pt nanoparticles toward HOR to an extent that has rarely been touched.
Bibliography:istex:16E8BFF7B064ACC65DAB0A52BFA26DE8829BA6CA
ark:/67375/TPS-NSQJD6XP-P
ObjectType-Article-1
SourceType-Scholarly Journals-1
ObjectType-Feature-2
content type line 23
ISSN:0002-7863
1520-5126
DOI:10.1021/ja076177b