Activation of 1.54 μm Er3+ Fluorescence in Concentrated II−VI Semiconductor Cluster Environments

A strong enhancement of the 1.54 μm fluorescence of Er3+ has been achieved in highly concentrated II−VI semiconductor quantum dot environments. A new preparation strategy allowed to incorporate up to 20 at. % Er3+ into ZnS, CdS, and CdSe as well as ZnO semiconductor clusters and nanocrystals (sizes...

Full description

Saved in:
Bibliographic Details
Published inChemistry of materials Vol. 10; no. 1; pp. 65 - 71
Main Authors Schmidt, Thomas, Müller, Gerd, Spanhel, Lubomir, Kerkel, Klaus, Forchel, Alfred
Format Journal Article
LanguageEnglish
Published Washington, DC American Chemical Society 19.01.1998
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A strong enhancement of the 1.54 μm fluorescence of Er3+ has been achieved in highly concentrated II−VI semiconductor quantum dot environments. A new preparation strategy allowed to incorporate up to 20 at. % Er3+ into ZnS, CdS, and CdSe as well as ZnO semiconductor clusters and nanocrystals (sizes 1.5−5 nm). All clusters investigated contain OH groups that serve as bridging ligands for the lanthanide attachment. Er3+ in ethanolic cluster solutions is fluorescing by 3 orders of magnitude more strongly than in pure ethanol, which can only be explained by a cagelike architecture of these clusters offering a large intake capacity. With this new material concept, the two well-known radiationless recombination channels related to electron−phonon coupling and Er−O−Er clustering can be controlled. First, with decreasing number of erbium ions per nanoparticle, the fluorescence intensity increases, approaching its maximum at 2 at. % Er3+. Second, it is shown that the fluorescence intensity increases with decreasing energy of phonons produced by lattice vibrations of the surrounding cluster carrier. For example, ethanolic molecular erbium/(aminopropyl)trialkoxysilane (AMEO) complexes exhibit the lowest fluorescence intensity of all samples employed, due to the presence of high-energy OH and NH vibrations (between 3000 and 3500 cm-1). Ethanolic Er/ZnO colloids, however, fluoresce 100 times more intense, which can be interpreted in terms of the lower phonon energy of the ZnO lattice vibrations (between 500 and 1000 cm-1). The AMEO-capped 1.6 nm CdSe/Er3+ clusters in ethanol fluoresce 1000 times more strongly than ethanolic AMEO/Er3+ complexes (CdSe phonon energies around 200 cm-1).
Bibliography:ark:/67375/TPS-DTX74G2T-M
istex:632E7E71FEC6AE2D7FE8C1126ED3F8EEA91F355D
ISSN:0897-4756
1520-5002
DOI:10.1021/cm9702169