Lithium-metal composite oxides and electrochemical device using the same
0ppm240ppm0ppm240ppm0ppm240ppm240ppm0ppmThe present invention relates to a lithium-containing metal composite oxide comprising paramagnetic and diamagnetic metals, which satisfies any one of the following conditions: (a) the ratio of intensity between a main peak of 0±10 ppm (I) and a main peak of 2...
Saved in:
Main Authors | , , , , , , , , , , |
---|---|
Format | Patent |
Language | English |
Published |
26.06.2012
|
Online Access | Get full text |
Cover
Loading…
Summary: | 0ppm240ppm0ppm240ppm0ppm240ppm240ppm0ppmThe present invention relates to a lithium-containing metal composite oxide comprising paramagnetic and diamagnetic metals, which satisfies any one of the following conditions: (a) the ratio of intensity between a main peak of 0±10 ppm (I) and a main peak of 240±140 ppm (I), (I/I), is less than 0.117·Z wherein z is the ratio of moles of the diamagnetic metal to moles of lithium; (b) the ratio of line width between the main peak of 0±10 ppm (I) and the main peak of 240±140 ppm (I), (W/W), is less than 21.45; and (c) both the conditions (a) and (b). The peaks of the lithium-containing metal composite oxide are obtained according to the 7Li-NMR measurement conditions and means disclosed herein. |
---|