Method for manufacturing (Li, Na, K)(Nb, Ta)O
3 3 3 A method for manufacturing (Li, Na, K)(Nb, Ta)Otype piezoelectric material having an improved relative dielectric constant and an electric-field-induced strain is provided. The method is a process in which a formed body of powder particles constituted of a composition of (Li, Na, K)(Nb, Ta)Ois...
Saved in:
Main Authors | , , |
---|---|
Format | Patent |
Language | English |
Published |
28.02.2012
|
Online Access | Get full text |
Cover
Loading…
Summary: | 3 3 3 A method for manufacturing (Li, Na, K)(Nb, Ta)Otype piezoelectric material having an improved relative dielectric constant and an electric-field-induced strain is provided. The method is a process in which a formed body of powder particles constituted of a composition of (Li, Na, K)(Nb, Ta)Ois fired to produce the (Li, Na, K)(Nb, Ta)Otype piezoelectric material, and a constant temperature is kept in a range of 850 to 1000° C. for a constant time before heating to a firing temperature. |
---|