Attenuated Total Reflectance was used to measure the phonon vibration frequencies over the range 425-800 cm(-1) of SrTiO (3) thin films deposited either directly on LaAlO(3), or on YBCO-coated LaAlO(3) single crystal substrates. In the s-polarized spectra, the transverse optic Ti-O stretching vibrat...
Saved in:
Published in | IEEE transactions on applied superconductivity Vol. 7; no. 2; pp. 1628 - 1631 |
---|---|
Main Authors | , , , , , , , |
Format | Journal Article |
Language | English |
Published |
01.06.1997
|
Online Access | Get full text |
Cover
Loading…
Summary: | Attenuated Total Reflectance was used to measure the phonon vibration frequencies over the range 425-800 cm(-1) of SrTiO (3) thin films deposited either directly on LaAlO(3), or on YBCO-coated LaAlO(3) single crystal substrates. In the s-polarized spectra, the transverse optic Ti-O stretching vibration shifted to lower frequencies as the film thickness increased, which was attributed to damping caused by the generation of lower frequency phonon modes. The transverse Ti-O stretching vibration was also observed in the p-polarized spectra, but was more heavily damped, which indicates the damping is more pronounced when the electric field has a component perpendicular to the film surface. Damping of the transverse modes was attributed to coupling of these modes to other phonon modes, and may be a source of the high losses at microwave frequencies |
---|---|
Bibliography: | ObjectType-Article-2 SourceType-Scholarly Journals-1 content type line 23 ObjectType-Feature-1 |
ISSN: | 1051-8223 |
DOI: | 10.1109/77.620889 |