Investigation of Degree of Undercooling of Fe-O Alloy on Al^sub 2^O3 Substrate
An Fe-O drop of ~0.4 g in an alumina crucible was quenched from ~2200 K (~1927 °C) at a cooling rate of -87 K/s by flowing He gas at a flow rate of 25 L/min STP. A deep undercooling of approximately 200 K was obtained regardless the oxygen content in the sample. According to the classical nucleation...
Saved in:
Published in | Metallurgical and materials transactions. B, Process metallurgy and materials processing science Vol. 45; no. 5; p. 1589 |
---|---|
Main Authors | , , , |
Format | Journal Article |
Language | English |
Published |
New York
Springer Nature B.V
01.10.2014
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | An Fe-O drop of ~0.4 g in an alumina crucible was quenched from ~2200 K (~1927 °C) at a cooling rate of -87 K/s by flowing He gas at a flow rate of 25 L/min STP. A deep undercooling of approximately 200 K was obtained regardless the oxygen content in the sample. According to the classical nucleation theory, the contact angle between a solid Fe nuclei and the Al^sub 2^O3 substrate was estimated to be 53 (±4) deg.[PUBLICATION ABSTRACT] |
---|---|
ISSN: | 1073-5615 1543-1916 |
DOI: | 10.1007/s11663-014-0166-0 |