METHOD FOR PRODUCING POSITIVE ELECTRODE SLURRY AND METHOD FOR PRODUCING POSITIVE ELECTRODE
This method for producing a positive electrode slurry comprises: a step wherein an aqueous solution, in which a smectite is dissolved, is mixed with a solvent containing N-methyl-2-pyrrolidone (NMP), thereby preparing an aqueous smectite-NMP solution; a step wherein the aqueous smectite-NMP solution...
Saved in:
Main Authors | , |
---|---|
Format | Patent |
Language | English French Japanese |
Published |
23.06.2022
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Abstract | This method for producing a positive electrode slurry comprises: a step wherein an aqueous solution, in which a smectite is dissolved, is mixed with a solvent containing N-methyl-2-pyrrolidone (NMP), thereby preparing an aqueous smectite-NMP solution; a step wherein the aqueous smectite-NMP solution is subjected to thermal dehydration, thereby obtaining a smectite-containing solid content lump; and a step wherein the smectite-containing solid content lump, a positive electrode active material and the solvent containing N-methyl-2-pyrrolidone (NMP) are mixed with each other, thereby preparing a slurry.
Ce procédé de production d'une suspension épaisse pour électrode positive comprend : une étape dans laquelle une solution aqueuse, dans laquelle est dissoute une smectite, est mélangée à un solvant contenant de la N-méthyl-2-pyrrolidone (NMP), ce qui permet de préparer une solution aqueuse de smectite-NMP ; une étape dans laquelle la solution aqueuse de smectite-NMP est soumise à une déshydratation thermique, ce qui permet d'obtenir une agglomération de matières solides contenant de la smectite ; et une étape dans laquelle l'agglomération de matières solides contenant de la smectite, un matériau actif d'électrode positive et le solvant contenant de la N-méthyl-2-pyrrolidone (NMP) sont mélangés les uns avec les autres, ce qui permet de préparer une suspension épaisse.
正極スラリーの製造方法は、スメクタイトが溶解した水溶液と、N-メチル-2-ピロリドン(NMP)含有溶媒とを混合して、スメクタイト-NMP水溶液を調製する工程と、前記スメクタイト-NMP水溶液を加熱脱水して、スメクタイト含有固形分塊を得る工程と、前記スメクタイト含有固形分塊と、正極活物質と、N-メチル-2-ピロリドン(NMP)含有溶媒とを混合してスラリーを調製する工程と、を有する。 |
---|---|
AbstractList | This method for producing a positive electrode slurry comprises: a step wherein an aqueous solution, in which a smectite is dissolved, is mixed with a solvent containing N-methyl-2-pyrrolidone (NMP), thereby preparing an aqueous smectite-NMP solution; a step wherein the aqueous smectite-NMP solution is subjected to thermal dehydration, thereby obtaining a smectite-containing solid content lump; and a step wherein the smectite-containing solid content lump, a positive electrode active material and the solvent containing N-methyl-2-pyrrolidone (NMP) are mixed with each other, thereby preparing a slurry.
Ce procédé de production d'une suspension épaisse pour électrode positive comprend : une étape dans laquelle une solution aqueuse, dans laquelle est dissoute une smectite, est mélangée à un solvant contenant de la N-méthyl-2-pyrrolidone (NMP), ce qui permet de préparer une solution aqueuse de smectite-NMP ; une étape dans laquelle la solution aqueuse de smectite-NMP est soumise à une déshydratation thermique, ce qui permet d'obtenir une agglomération de matières solides contenant de la smectite ; et une étape dans laquelle l'agglomération de matières solides contenant de la smectite, un matériau actif d'électrode positive et le solvant contenant de la N-méthyl-2-pyrrolidone (NMP) sont mélangés les uns avec les autres, ce qui permet de préparer une suspension épaisse.
正極スラリーの製造方法は、スメクタイトが溶解した水溶液と、N-メチル-2-ピロリドン(NMP)含有溶媒とを混合して、スメクタイト-NMP水溶液を調製する工程と、前記スメクタイト-NMP水溶液を加熱脱水して、スメクタイト含有固形分塊を得る工程と、前記スメクタイト含有固形分塊と、正極活物質と、N-メチル-2-ピロリドン(NMP)含有溶媒とを混合してスラリーを調製する工程と、を有する。 |
Author | TOKIEDA Daisuke MINO Shinji |
Author_xml | – fullname: MINO Shinji – fullname: TOKIEDA Daisuke |
BookMark | eNrjYmDJy89L5WSI8nUN8fB3UXDzD1IICPJ3CXX29HNXCPAP9gzxDHNVcPVxdQ4BCrsqBPuEBgVFKjj6uSgQqYWHgTUtMac4lRdKczMou7mGOHvophbkx6cWFyQmp-allsSH-xsZGBkZGhuYm1g6GhoTpwoAj_s0yQ |
ContentType | Patent |
DBID | EVB |
DatabaseName | esp@cenet |
DatabaseTitleList | |
Database_xml | – sequence: 1 dbid: EVB name: esp@cenet url: http://worldwide.espacenet.com/singleLineSearch?locale=en_EP sourceTypes: Open Access Repository |
DeliveryMethod | fulltext_linktorsrc |
Discipline | Medicine Chemistry Sciences |
DocumentTitleAlternate | 正極スラリーの製造方法及び正極の製造方法 PROCÉDÉ DE PRODUCTION DE SUSPENSION ÉPAISSE POUR ÉLECTRODE POSITIVE ET PROCÉDÉ DE PRODUCTION D'ÉLECTRODE POSITIVE |
ExternalDocumentID | WO2022130749A1 |
GroupedDBID | EVB |
ID | FETCH-epo_espacenet_WO2022130749A13 |
IEDL.DBID | EVB |
IngestDate | Fri Jul 19 12:55:46 EDT 2024 |
IsOpenAccess | true |
IsPeerReviewed | false |
IsScholarly | false |
Language | English French Japanese |
LinkModel | DirectLink |
MergedId | FETCHMERGED-epo_espacenet_WO2022130749A13 |
Notes | Application Number: WO2021JP37375 |
OpenAccessLink | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20220623&DB=EPODOC&CC=WO&NR=2022130749A1 |
ParticipantIDs | epo_espacenet_WO2022130749A1 |
PublicationCentury | 2000 |
PublicationDate | 20220623 |
PublicationDateYYYYMMDD | 2022-06-23 |
PublicationDate_xml | – month: 06 year: 2022 text: 20220623 day: 23 |
PublicationDecade | 2020 |
PublicationYear | 2022 |
RelatedCompanies | PANASONIC INTELLECTUAL PROPERTY MANAGEMENT CO., LTD |
RelatedCompanies_xml | – name: PANASONIC INTELLECTUAL PROPERTY MANAGEMENT CO., LTD |
Score | 3.5355623 |
Snippet | This method for producing a positive electrode slurry comprises: a step wherein an aqueous solution, in which a smectite is dissolved, is mixed with a solvent... |
SourceID | epo |
SourceType | Open Access Repository |
SubjectTerms | BASIC ELECTRIC ELEMENTS ELECTRICITY PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY |
Title | METHOD FOR PRODUCING POSITIVE ELECTRODE SLURRY AND METHOD FOR PRODUCING POSITIVE ELECTRODE |
URI | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20220623&DB=EPODOC&locale=&CC=WO&NR=2022130749A1 |
hasFullText | 1 |
inHoldings | 1 |
isFullTextHit | |
isPrint | |
link | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwjV1RT8IwEL4QNOqbokYUTRPN3hYZG1AeiIG2uBnYljEQfSHrVhKNASIz_n1vCyhPxLe2lzbtpd9dv7bXAtwlSYQWgErdSGisW7IudSpjiXPZUI2MD8hWFpw8cBv2yHqa1CcF-NjEwuTvhH7njyMiomLEe5rb6-XfJhbP71au7uUbFi0eemGba2t2XKtV0Z1rvNsWvsc9pjGGvE1zg1yG5rpptTrIlfZwId3M8CDG3SwuZbntVHrHsO9je_P0BArvUQkO2ebvtRIcDNZH3phco291Cq8DEdoeJ0jciB94fMQc95H43tAJnbEgoi9YiMWCDPujIHghHZeTf1Y5g9ueCJmtYyenvzqZPnvbIzLPoThfzNUFEKpMOktwXWMo05pRM7KqNKnH1UgqQxmxKkNlV0uXu8VXcJRls7tSNbMCxfTzS12jV07lTa7MHxQQicI |
link.rule.ids | 230,309,783,888,25576,76882 |
linkProvider | European Patent Office |
linkToHtml | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwjV3dT8IwEL8QNeKbosYP1CaavS0yNrA8EANdcdN9ZQxEX8i6lURjgMiM_763BZQn4lvTSy_tpffxa3s9gJs0jdECUKFqKU1UQzSESkUicC9rspnjAdHKk5Ndr2kNjMdRY1SCj1UuTPFP6HfxOSJqVIL6nhX2ev53iGUWbysXt-INu2b3vahtKkt0XK_X0J0rZrfNA9_0mcIY4jbFCwsamus7o9VBrLSNQTbN6x3wYTfPS5mvO5XePuwEyG-aHUDpPa5Ama1qr1Vg111eeWNzqX2LQ3h1eWT5JkHgRoLQNwfM9h5I4PftyB5ywh3OIuzmpO8MwvCFdDyT_HPIEVz3eMQsFSc5_pXJ-NlfX5F-DFvT2VSeAKFSp5MU4xpN6saE6rFRo2kjqcVCalJL5ClUN3E620y-grIVuc7Ysb2nc9jLSfm7qbpeha3s80teoIfOxGUh2B-ymoyy |
openUrl | ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Apatent&rft.title=METHOD+FOR+PRODUCING+POSITIVE+ELECTRODE+SLURRY+AND+METHOD+FOR+PRODUCING+POSITIVE+ELECTRODE&rft.inventor=MINO+Shinji&rft.inventor=TOKIEDA+Daisuke&rft.date=2022-06-23&rft.externalDBID=A1&rft.externalDocID=WO2022130749A1 |