BEARING STEEL MATERIAL WITH EXCELLENT ROLLING FATIGUE PROPERTY AND BEARING PART
A bearing steel material which contains 0.8-1.1 mass% C, 0.15-0.8 mass% Si, 0.1-1.0 mass% Mn, 1.3-1.8 mass% Cr, up to 0.05 mass% P (0 mass% is excluded), up to 0.015 mass% S (0 mass% is excluded), 0.0002-0.005 mass% Al, 0.0002-0.0020 mass% Ca, 0.0005-0.010 mass% Ti, up to 0.0080 mass% N (0 mass% is...