MQ resins from stable ethylsilicate polymers
An MQ resin including at least 30% SiO2, preferably at least 50 wt % SiO2, and having dynamic viscosity of 50 centipoises (cps) to 750 cps at 25° C. is produced from a stable ethylsilicate polymer. The ethylsilicate polymer includes not greater than 1 wt % of TEOS monomer. The ethylsilicate polymer...
Saved in:
Main Authors | , , , |
---|---|
Format | Patent |
Language | English |
Published |
09.09.2014
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | An MQ resin including at least 30% SiO2, preferably at least 50 wt % SiO2, and having dynamic viscosity of 50 centipoises (cps) to 750 cps at 25° C. is produced from a stable ethylsilicate polymer. The ethylsilicate polymer includes not greater than 1 wt % of TEOS monomer. The ethylsilicate polymer is produced by a two step addition of catalysts wherein a hydrolysis catalyst, for example, hydrochloric acid is added initially and a second catalyst, such as phosphonitrilic chloride trimer, is added subsequently. |
---|---|
Bibliography: | Application Number: US20110983540 |