High flexible propylene/ethylene copolymers and process for preparing same

Highly flexible propylene/ethylene copolymers having a high rubber content are obtainable by two-stage polymerization from the gas phase in an agitated fixed bed by means of a Ziegler-Natta catalyst system which, in addition to a titanium-containing solid component, also contains an aluminum compoun...

Full description

Saved in:
Bibliographic Details
Main Authors KERSTING; MEINOLF, MUELLER; PATRIK
Format Patent
LanguageEnglish
Published 21.04.1998
Edition6
Subjects
Online AccessGet full text

Cover

Loading…
Abstract Highly flexible propylene/ethylene copolymers having a high rubber content are obtainable by two-stage polymerization from the gas phase in an agitated fixed bed by means of a Ziegler-Natta catalyst system which, in addition to a titanium-containing solid component, also contains an aluminum compound as a cocatalyst, in a first polymerization stage, propylene being polymerized at from 15 to 40 bar and from 50 DEG to 90 DEG C. and during an average residence time of the reaction mixture of from 0.5 to 5 hours and then, in a second polymerization stage, a mixture of propylene and ethylene being polymerized with the polymer discharged from the first polymerization stage, at from 5 to 30 bar, this pressure being at least 2 bar below the pressure of the first polymerization stage, and at from 60 DEG to 100 DEG C. and during an average residence time of the reaction mixture of from 0.5 to 5 hours, the ratio of the partial pressure of propylene to that of ethylene being brought within the range from 0.5: to 5:1, the weight ratio of the monomers reacted in the first polymerization stage to those reacted in the second polymerization stage being from 0.9:1 to 0.4:1 and the polymerization in the second polymerization stage being carried out in the presence of a C1-C8-alkanol.
AbstractList Highly flexible propylene/ethylene copolymers having a high rubber content are obtainable by two-stage polymerization from the gas phase in an agitated fixed bed by means of a Ziegler-Natta catalyst system which, in addition to a titanium-containing solid component, also contains an aluminum compound as a cocatalyst, in a first polymerization stage, propylene being polymerized at from 15 to 40 bar and from 50 DEG to 90 DEG C. and during an average residence time of the reaction mixture of from 0.5 to 5 hours and then, in a second polymerization stage, a mixture of propylene and ethylene being polymerized with the polymer discharged from the first polymerization stage, at from 5 to 30 bar, this pressure being at least 2 bar below the pressure of the first polymerization stage, and at from 60 DEG to 100 DEG C. and during an average residence time of the reaction mixture of from 0.5 to 5 hours, the ratio of the partial pressure of propylene to that of ethylene being brought within the range from 0.5: to 5:1, the weight ratio of the monomers reacted in the first polymerization stage to those reacted in the second polymerization stage being from 0.9:1 to 0.4:1 and the polymerization in the second polymerization stage being carried out in the presence of a C1-C8-alkanol.
Author KERSTING; MEINOLF
MUELLER; PATRIK
Author_xml – fullname: KERSTING; MEINOLF
– fullname: MUELLER; PATRIK
BookMark eNrjYmDJy89L5WTw8shMz1BIy0mtyEzKSVUoKMovqMxJzUvVTy3JADMUkvML8nMqc1OLihUS81JAKpJTi4sV0vKLgOzUgsSizLx0heLE3FQeBta0xJziVF4ozc0g7-Ya4uyhm1qQH59aXJCYDDSuJD402NTcxNDCzMjRmLAKALs9NsU
ContentType Patent
DBID EVB
DatabaseName esp@cenet
DatabaseTitleList
Database_xml – sequence: 1
  dbid: EVB
  name: esp@cenet
  url: http://worldwide.espacenet.com/singleLineSearch?locale=en_EP
  sourceTypes: Open Access Repository
DeliveryMethod fulltext_linktorsrc
Discipline Medicine
Chemistry
Sciences
Edition 6
ExternalDocumentID US5741862A
GroupedDBID EVB
ID FETCH-epo_espacenet_US5741862A3
IEDL.DBID EVB
IngestDate Fri Jul 19 14:25:22 EDT 2024
IsOpenAccess true
IsPeerReviewed false
IsScholarly false
Language English
LinkModel DirectLink
MergedId FETCHMERGED-epo_espacenet_US5741862A3
Notes Application Number: US19970782085
OpenAccessLink https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19980421&DB=EPODOC&CC=US&NR=5741862A
ParticipantIDs epo_espacenet_US5741862A
PublicationCentury 1900
PublicationDate 19980421
PublicationDateYYYYMMDD 1998-04-21
PublicationDate_xml – month: 04
  year: 1998
  text: 19980421
  day: 21
PublicationDecade 1990
PublicationYear 1998
RelatedCompanies BASF AKTIENGESELLSCHAFT
RelatedCompanies_xml – name: BASF AKTIENGESELLSCHAFT
Score 2.487719
Snippet Highly flexible propylene/ethylene copolymers having a high rubber content are obtainable by two-stage polymerization from the gas phase in an agitated fixed...
SourceID epo
SourceType Open Access Repository
SubjectTerms CHEMISTRY
COMPOSITIONS BASED THEREON
MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
Title High flexible propylene/ethylene copolymers and process for preparing same
URI https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19980421&DB=EPODOC&locale=&CC=US&NR=5741862A
hasFullText 1
inHoldings 1
isFullTextHit
isPrint
link http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwdV3PS8MwFH7MKepNpzJ_5yC9hdk17eyhiOsPxsBtuFV2G0uTqqBZsRXZf-9Lt6qX3R4phCTk5ctL3_c9gBtmzrVMpaBJhzHKEGAo546kt6nNuED84bxMkB04vZj1p_a0Bq8VF6bUCf0uxRHRoxL096I8r7O_R6ygzK3MW_wNmxb30cQLDFHRxXAPmkbQ9cLRMBj6hu978dgYPHm2Vmlx2g9bsK0v0VplP3zuak5K9h9QogPYGWFfqjiEmlQN2POrumsN2H1c_-5Gc-15-RH0dUIGSbV8JX-XBM-9bImAIVsSV1obJNHlDpb6GZrMlSDZigFA8FKKttTFBtULyecf8hiuo3Di9ygOavY7_1k8rkZvnUBdLZRsAsFQSWitMu5ggOZ23DtLWkI4LEUHczHsO4Xmpl7ONn86h_0V6Y7RtnkB9eLzS14i6hb8qlywH7X0iBU
link.rule.ids 230,309,786,891,25594,76903
linkProvider European Patent Office
linkToHtml http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwdV1NT8JAEJ0gGvGmqMFP9mB6a7CwFHtojLSQinxFqOFGWHaLJro0tsbw751dqHrhNmmTzXbT2de3nfcG4IZaM2VTyc15g1KTIsCYjNnCvI3qlHHEH8Z0gWzfDkLamdQnOXjNtDDaJ_RbmyNiRs0x31O9X8d_h1i-rq1MKuwNLy3v22PXN3gmF8N30DL8ptsaDvyBZ3ieG46M_rNbVy4tdvVhB3YbSAg1UXppKk1K_B9Q2oewN8SxZHoEOSGLUPCyvmtF2O9tfndjuMm85Bg6qiCDRMq-kr0LgvtevELAEBWBK60CMlftDlbqGJrMJCfxWgFA8KMUY6GaDcoFSWYf4gTK7dbYC0yc1PT3-afhKJt97RTycilFCQhSJa68ypiNBM1pOHc1UePcphEmmIO07wxK20Y5336rDIVg3OtOu4_9pws4WAvwqFm1LiGffn6JK0TglF3rxfsBN12K_w
openUrl ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Apatent&rft.title=High+flexible+propylene%2Fethylene+copolymers+and+process+for+preparing+same&rft.inventor=KERSTING%3B+MEINOLF&rft.inventor=MUELLER%3B+PATRIK&rft.date=1998-04-21&rft.externalDBID=A&rft.externalDocID=US5741862A