Process for the production of composite safety glass

An improvement in a method for manufacturing a composite safety glass wherein one or more silicate glass panes is bonded to a plasticized synthetic resin film at an elevated temperature, the improvement residing in employing as the plasticized synthetic resin film a soft film of a polymer of ethylen...

Full description

Saved in:
Bibliographic Details
Main Authors KNACKSTEDT; WILHELM, BECKMANN; ROLF
Format Patent
LanguageEnglish
Published 28.08.1990
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:An improvement in a method for manufacturing a composite safety glass wherein one or more silicate glass panes is bonded to a plasticized synthetic resin film at an elevated temperature, the improvement residing in employing as the plasticized synthetic resin film a soft film of a polymer of ethylene and/or propylene and effecting the bonding under pressure at a temperature of at least 120 DEG C. and up to 200 DEG C.
Bibliography:Application Number: US19890367912