Process for the production of fiber-grade terephthalic acid
Process for the preparation of fiber-grade terephthalic acid by continuously oxidizing paraxylene while vaporizing a portion of the contents of the reactor. Fiber-grade terephthalic acid is produced by maintaining (1) a temperature of at least 210 DEG C., (2) a molecular oxygen content of the noncon...