METHOD OF USING HIGH MOLECULAR WEIGHT AROMATIC POLYOL POLYESTERS AS DEMULSIFIERS FOR CRUDE OIL TREATMENT
A method of demulsifying crude oil, said method comprising the step of reacting an amount of crude oil with a polyester demulsifier, therein the demulsifier is used in quantities from 0.0001% to 5% (1-50,000 ppm), preferably 0.0005% to 2% (5-20,000 ppm), more preferably 0.0008% to 1% (8-10,000 ppm)...
Saved in:
Main Authors | , , |
---|---|
Format | Patent |
Language | English |
Published |
19.11.2020
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | A method of demulsifying crude oil, said method comprising the step of reacting an amount of crude oil with a polyester demulsifier, therein the demulsifier is used in quantities from 0.0001% to 5% (1-50,000 ppm), preferably 0.0005% to 2% (5-20,000 ppm), more preferably 0.0008% to 1% (8-10,000 ppm) and most preferably 0.001 to 0.1 wt. % polymer (10-1,000 ppm) related to the oil fraction of the utilized emulsion. |
---|---|
Bibliography: | Application Number: US201816763839 |