Rubber composition comprising a specific hydrocarbon resin
A rubber composition is based on at least: from 60 to 100 phr of one or more diene elastomers, referred to as very low glass transition temperature (Tg) diene elastomers, exhibiting a Tg within a range extending from −110° C. to −70° C., chosen from butadiene homopolymers, copolymers of butadiene an...