METHOD OF TIGHT BONDING OF GLASS CERAMICS WITH METAL PART
FIELD: process engineering.SUBSTANCE: invention relates to laser engineering, particularly, to laser gyroscopy. Metal part is placed on glass ceramics block. Bulge is made between surfaces to be bonded together by straying powder at angle of 75-90 degrees to bond surface. Block with part are placed...
Saved in:
Main Authors | , , , , |
---|---|
Format | Patent |
Language | English Russian |
Published |
20.06.2013
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Abstract | FIELD: process engineering.SUBSTANCE: invention relates to laser engineering, particularly, to laser gyroscopy. Metal part is placed on glass ceramics block. Bulge is made between surfaces to be bonded together by straying powder at angle of 75-90 degrees to bond surface. Block with part are placed in kiln heated to 400-450°C and exposed for, at least, one hour. Then, its is cooled to room temperature at the rate of, at least, 5 °C/min.EFFECT: higher precision and safety of annular laser gyroscope.
Изобретение относится к лазерной технике, а именно к лазерной гироскопии. Металлическую деталь устанавливают на стеклокерамический блок. Между соединяемыми поверхностями создают валик путем напыления порошка под углом 75-90° по отношению к создаваемому соединению. Блок с деталью устанавливают в печь, нагретую до температуры 400-450°С, выдерживают не менее 1 часа и охлаждают до комнатной температуры со скоростью не более 5°С/мин. Обеспечивается повышение точности и сохраняемости кольцевого лазерного гироскопа. |
---|---|
AbstractList | FIELD: process engineering.SUBSTANCE: invention relates to laser engineering, particularly, to laser gyroscopy. Metal part is placed on glass ceramics block. Bulge is made between surfaces to be bonded together by straying powder at angle of 75-90 degrees to bond surface. Block with part are placed in kiln heated to 400-450°C and exposed for, at least, one hour. Then, its is cooled to room temperature at the rate of, at least, 5 °C/min.EFFECT: higher precision and safety of annular laser gyroscope.
Изобретение относится к лазерной технике, а именно к лазерной гироскопии. Металлическую деталь устанавливают на стеклокерамический блок. Между соединяемыми поверхностями создают валик путем напыления порошка под углом 75-90° по отношению к создаваемому соединению. Блок с деталью устанавливают в печь, нагретую до температуры 400-450°С, выдерживают не менее 1 часа и охлаждают до комнатной температуры со скоростью не более 5°С/мин. Обеспечивается повышение точности и сохраняемости кольцевого лазерного гироскопа. |
Author | GOLJAEV JURIJ DMITRIEVICH NEDZVETSKAJA ALEKSANDRA ANATOL'EVNA KRYLOVA GALINA VIKTOROVNA POLEKHIN IVAN NIKOLAEVICH ZAPOTYL'KO NINA RUDOL'FOVNA |
Author_xml | – fullname: KRYLOVA GALINA VIKTOROVNA – fullname: ZAPOTYL'KO NINA RUDOL'FOVNA – fullname: NEDZVETSKAJA ALEKSANDRA ANATOL'EVNA – fullname: POLEKHIN IVAN NIKOLAEVICH – fullname: GOLJAEV JURIJ DMITRIEVICH |
BookMark | eNrjYmDJy89L5WSw9HUN8fB3UfB3UwjxdPcIUXDy93Px9HMHCbj7OAYHKzi7Bjn6ejoHK4R7hngoAJU7-igEOAaF8DCwpiXmFKfyQmluBgU31xBnD93Ugvz41OKCxOTUvNSS-KBQIxMLE0tjA2dDYyKUAAAV4Cnd |
ContentType | Patent |
DBID | EVB |
DatabaseName | esp@cenet |
DatabaseTitleList | |
Database_xml | – sequence: 1 dbid: EVB name: esp@cenet url: http://worldwide.espacenet.com/singleLineSearch?locale=en_EP sourceTypes: Open Access Repository |
DeliveryMethod | fulltext_linktorsrc |
Discipline | Medicine Chemistry Sciences |
DocumentTitleAlternate | СПОСОБ ГЕРМЕТИЧНОГО СОЕДИНЕНИЯ СТЕКЛОКЕРАМИКИ С МЕТАЛЛИЧЕСКОЙ ДЕТАЛЬЮ |
ExternalDocumentID | RU2484930C1 |
GroupedDBID | EVB |
ID | FETCH-epo_espacenet_RU2484930C13 |
IEDL.DBID | EVB |
IngestDate | Fri Jul 19 12:32:35 EDT 2024 |
IsOpenAccess | true |
IsPeerReviewed | false |
IsScholarly | false |
Language | English Russian |
LinkModel | DirectLink |
MergedId | FETCHMERGED-epo_espacenet_RU2484930C13 |
Notes | Application Number: RU20120116435 |
OpenAccessLink | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20130620&DB=EPODOC&CC=RU&NR=2484930C1 |
ParticipantIDs | epo_espacenet_RU2484930C1 |
PublicationCentury | 2000 |
PublicationDate | 20130620 |
PublicationDateYYYYMMDD | 2013-06-20 |
PublicationDate_xml | – month: 06 year: 2013 text: 20130620 day: 20 |
PublicationDecade | 2010 |
PublicationYear | 2013 |
RelatedCompanies | FEDERAL'NOE GOSUDARSTVENNOE UNITARNOE PREDPRIJATIE "NAUCHNO-ISSLEDOVATEL'SKIJ INSTITUT "POLJUS" IM.M.F. STEL'MAKHA (FGUP NII "POLJUS" IM. M.F. STEL'MAKHA) |
RelatedCompanies_xml | – name: FEDERAL'NOE GOSUDARSTVENNOE UNITARNOE PREDPRIJATIE "NAUCHNO-ISSLEDOVATEL'SKIJ INSTITUT "POLJUS" IM.M.F. STEL'MAKHA (FGUP NII "POLJUS" IM. M.F. STEL'MAKHA) |
Score | 2.891327 |
Snippet | FIELD: process engineering.SUBSTANCE: invention relates to laser engineering, particularly, to laser gyroscopy. Metal part is placed on glass ceramics block.... |
SourceID | epo |
SourceType | Open Access Repository |
SubjectTerms | CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS CHEMISTRY CLADDING OR PLATING BY SOLDERING OR WELDING CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING GLASS JOINING GLASS TO GLASS OR OTHER MATERIALS MACHINE TOOLS METAL-WORKING NOT OTHERWISE PROVIDED FOR METALLURGY MINERAL OR SLAG WOOL PERFORMING OPERATIONS SOLDERING OR UNSOLDERING SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS SURFACE TREATMENT OF GLASS TRANSPORTING WELDING WORKING BY LASER BEAM |
Title | METHOD OF TIGHT BONDING OF GLASS CERAMICS WITH METAL PART |
URI | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20130620&DB=EPODOC&locale=&CC=RU&NR=2484930C1 |
hasFullText | 1 |
inHoldings | 1 |
isFullTextHit | |
isPrint | |
link | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfR3LTsJAcELQqDdFjeAjezC9EfuGHhoD2xcGWlKKciPdsiRcCoESf9_ZWtCL3jazm8nsbOa1uzMD8KyY3OAZxyBnicegK9xsWwaXhSOXZqlhGSoT-c6j0Aym-tvMmNVgdciFKeuEfpbFEVGiMpT3otTXm59LLKf8W7l7YSsErV-9xHakKjpGhWyqsuT0bXccORGVKLXjqRTGtqp3dUuTKQZKJ8KLFmX23fe-SErZ_LYo3iWcjhFZXlxBbbtvwDk9NF5rwNmoeu_GYSV6u2uwRm4SRA6JPJIM_CAh_Sh0BqEvAP6wN5kQ6sY90ZKQfAySgODy3pCM0V-9AeK5CQ3aSMP8uN95PD1Sq91CPV_n_A5IimxTOGcdmTGdpV1L7cgLtM7mUtHMTFs0ofknmtY_c_dwoX63eECJeYB6sd3zRzS0BXsqWfQFWjp83Q |
link.rule.ids | 230,309,786,891,25594,76906 |
linkProvider | European Patent Office |
linkToHtml | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfR3LTsJAcELQiDdFjfjcg-mN2HfpoTGwbWm1D1IW5UbasiRcgECJv--0AnrR22Z2M5mdzbx2d2YAniSdazznGOTM8BhUiettU-Ni6cileaqZmpyV-c5hpHsj9XWsjWsw3-fCVHVCP6viiChROcp7Uenr1c8lll39rdw8Z3MELV9cZtnCLjpGhazLomD3LGcQ2zEVKLWSkRAllqx2VFMRKQZKR0ZZnLf0nN57ZVLK6rdFcc_geIDIFsU51NbbJjTovvFaE07C3Xs3Dneit7kAM3SYF9skdgnz-x4jvTiy_ahfAvpBdzgk1Em6ZUtC8uEzj-DybkAG6K9eAnEdRr020jA57HeSjA7UKldQXywX_BpIimyTOM8MMcvULO2YsiFO0TrrM0nRc2XagtafaG7-mXuEhsfCYBL40dstnMrf7R5Qeu6gXqy3_B6NbpE9VOz6AlmGf8o |
openUrl | ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Apatent&rft.title=METHOD+OF+TIGHT+BONDING+OF+GLASS+CERAMICS+WITH+METAL+PART&rft.inventor=KRYLOVA+GALINA+VIKTOROVNA&rft.inventor=ZAPOTYL%27KO+NINA+RUDOL%27FOVNA&rft.inventor=NEDZVETSKAJA+ALEKSANDRA+ANATOL%27EVNA&rft.inventor=POLEKHIN+IVAN+NIKOLAEVICH&rft.inventor=GOLJAEV+JURIJ+DMITRIEVICH&rft.date=2013-06-20&rft.externalDBID=C1&rft.externalDocID=RU2484930C1 |