METHOD FOR THERMORADIATION TREATMENT OF POLYTETRAFLUOROETHYLENE PRODUCTS

FIELD: polymer materials. SUBSTANCE: method consists in gamma-irradiation of product at elevated temperature in melt in inert medium. Melt is first cooled and irradiation is carried out until dose 5-35 Mrad is absorbed, while temperature of product is reduced during irradiation procedure by 0.8- 1 C...

Full description

Saved in:
Bibliographic Details
Main Authors SOBOLEV G.P, BRUK M.A, IVANCHENKO V.K, SICHKAR' V.P, KHATIPOV S.A, VORONINA E.N
Format Patent
LanguageEnglish
Published 27.08.2003
Edition7
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:FIELD: polymer materials. SUBSTANCE: method consists in gamma-irradiation of product at elevated temperature in melt in inert medium. Melt is first cooled and irradiation is carried out until dose 5-35 Mrad is absorbed, while temperature of product is reduced during irradiation procedure by 0.8- 1 C per 1 Mrad so that temperature of product is maintained below melting temperature of polytetrafluoroethylene but above crystallization temperature. EFFECT: decreased creeping and increased wear resistance of products at the same coefficient of fiction characteristic of polytetrafluoroethylene non-modified by radiation. 2 cl, 1 dwg, 1 tbl, 5 ex
Bibliography:Application Number: RU20010104473