AUSTENITIC STEEL HAVING SUPERIORCHARACTERISTIC IN RESIS TANCE AGAINST STRESS COROSION CRACKING METHOD FOR PRODUCING OF THE SAME AND USAGE OF THE SAME GOOD

The present invention relates to an austenitic steel comprising Ni of 9 - 30 %, Cr of 10 - 23 %, and Fe of at least 45 %, which is characterized in comprising enough Cr and Ni to form whole austenitic structure in the equilibrium diagram at 700 DEG C, having austenitic phase at room temperature, and...

Full description

Saved in:
Bibliographic Details
Main Authors KETA, SHINJU, AONO, YASUHISA, KATO, TAKAHIKO, SATO, HISASHI, YOSHINARI, AKIRA, IZUMIYA, MASAKIYO, KOTAMA, HITEYO, YAMAMOTO, MICHIYOSHI
Format Patent
LanguageEnglish
Korean
Published 13.06.1995
Edition6
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The present invention relates to an austenitic steel comprising Ni of 9 - 30 %, Cr of 10 - 23 %, and Fe of at least 45 %, which is characterized in comprising enough Cr and Ni to form whole austenitic structure in the equilibrium diagram at 700 DEG C, having austenitic phase at room temperature, and said austenitic phase is a single crystal, and has superior resistance against stress corrosion cracking. The austenitic steel is preferably comprising C </= 0.1 %, Si </= 1 %, Mn </= 2 %, Ni 9 - 15 %, Cr 16 - 18.5 %, and at least one of elements selected from the group of Mo 1 - 3 %, Ti 0.05 - 1 %, and Nb 0.1 - 1.5 %, as of an alloy composition. The alloy relating to the present invention is preferable as a material for members of a reactor core of a nuclear reactor.