PROCESS FOR PRODUCTION OF UNIDIRECTIONAL ELECTROMAGNETIC STEEL SHEET
In a method of manufacturing a grain-oriented electrical steel sheet including a nitriding treatment (step S7) and adopting so-called "low-temperature slab heating", the finish temperature of finish rolling in hot rolling (step S2) is set to 950°C or below, the cooling is started within 2...