COLORED EXTERNAL PARTS OF TITANIUM OR TITANIUM ALLOY

PURPOSE:To produce external parts which are hard and are resistant to staining by forming a glassy coating film formed of a liquid mixture composed of specific ratios of sodium silicate and silica sol as a protection for a thin film of a Ti metal which is electrolytically colored by anodic oxidation...

Full description

Saved in:
Bibliographic Details
Main Author SHIBAZAKI YASUO
Format Patent
LanguageEnglish
Published 09.01.1988
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:PURPOSE:To produce external parts which are hard and are resistant to staining by forming a glassy coating film formed of a liquid mixture composed of specific ratios of sodium silicate and silica sol as a protection for a thin film of a Ti metal which is electrolytically colored by anodic oxidation. CONSTITUTION:An agent for forming a film colorable by anodic oxidation formed by adding >=1 kinds of inorg. compd. selected from 10-60g/l Na2MoO4.2 H2O, 10-60g/l (NH4)2HPO4, and 5-30g/l NaF to water is prepd. The anodically oxidized film of the Ti or Ti alloy is electrolytically colored by using such electrolyte and applying 5-90V DC thereto at <=50 deg.C. The liquid mixture composed of the sodium silicate and silica sol at 5-10/1 mixing ratio (glassy film) is thereafter coated on the surface thereof and is dried to form the hard protective film on the surface colored by the anodic oxidation.
Bibliography:Application Number: JP19860146739