POLYESTER RESIN COMPOSITION FOR INJECTION MOLDING AND INJECITON MOLDED ARTICLE
PURPOSE:To decrease melt viscosity and improve processability without decreas ing mol.wt. by compounding a polyester resin for injection molding with a specific compd. CONSTITUTION:1 mol of pyromellitic dianhydride is reacted with about 2 mol of 12-28C alkylamine to give a bisamide compd., which is...
Saved in:
Main Authors | , , |
---|---|
Format | Patent |
Language | English |
Published |
13.11.1992
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | PURPOSE:To decrease melt viscosity and improve processability without decreas ing mol.wt. by compounding a polyester resin for injection molding with a specific compd. CONSTITUTION:1 mol of pyromellitic dianhydride is reacted with about 2 mol of 12-28C alkylamine to give a bisamide compd., which is condensed by dehydration to give a compd. of the formula wherein R is 12-28C linear or branched alkyl. 100 pts.wt. polyester resin for injection (pref. polyethylene or polybutylene terephthalate) is compounded with 0.1-20 pts.wt. compd. of the formula to give the title compsn., which is injection molded. |
---|---|
Bibliography: | Application Number: JP19910097209 |