FOAM-MOLDED PRODUCT, METHOD OF MANUFACTURING FOAM-MOLDED PRODUCT, AND METHOD OF SUPPRESSING POOR APPEARANCE OF FOAM-MOLDED PRODUCT
To provide a foam-molded product in which poor appearance such as pockmarks and swirls are suppressed, a method of manufacturing a foam-molded product capable of suppressing poor appearance of the foam-molded product, and a method of suppressing poor appearance of the form-molded product.SOLUTION: T...
Saved in:
Main Authors | , , , , , |
---|---|
Format | Patent |
Language | English Japanese |
Published |
08.06.2023
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Abstract | To provide a foam-molded product in which poor appearance such as pockmarks and swirls are suppressed, a method of manufacturing a foam-molded product capable of suppressing poor appearance of the foam-molded product, and a method of suppressing poor appearance of the form-molded product.SOLUTION: There are provided: a foam-molded product including a foam layer, and a skin layer covering the foam layer, wherein a maximum diameter of bubbles in the foam layer is 0.50 mm or less, in the foam layer, an average diameter of the bubbles measured in a same cross section as a maximum diameter of the bubbles is 0.05 mm to 0.15 mm and the bubbles having the maximum diameter and the average diameter are formed by thermal decomposition of a blowing agent; a method for manufacturing a foam-molded product; and a method for suppressing an appearance defect of a foam-molded product.SELECTED DRAWING: Figure 2
【課題】アバタ、スワール等の外観不良が抑制された発泡成形体、成形体の外観不良を抑制することが可能な発泡成形体の製造方法、及び発泡成形体の外観不良の抑制方法を提供する。【解決手段】発泡層と、前記発泡層を被覆するスキン層と、を備え、前記発泡層における気泡の最大径が0.50mm以下であり、前記発泡層における、前記気泡の最大径と同一断面で測定される気泡の平均径が0.05mm~0.15mmであり、前記最大径及び前記平均径を有する前記気泡は発泡剤の熱分解により形成される気泡である、発泡成形体;及び、発泡成形体の製造方法又は外観不良の抑制方法。【選択図】図2 |
---|---|
AbstractList | To provide a foam-molded product in which poor appearance such as pockmarks and swirls are suppressed, a method of manufacturing a foam-molded product capable of suppressing poor appearance of the foam-molded product, and a method of suppressing poor appearance of the form-molded product.SOLUTION: There are provided: a foam-molded product including a foam layer, and a skin layer covering the foam layer, wherein a maximum diameter of bubbles in the foam layer is 0.50 mm or less, in the foam layer, an average diameter of the bubbles measured in a same cross section as a maximum diameter of the bubbles is 0.05 mm to 0.15 mm and the bubbles having the maximum diameter and the average diameter are formed by thermal decomposition of a blowing agent; a method for manufacturing a foam-molded product; and a method for suppressing an appearance defect of a foam-molded product.SELECTED DRAWING: Figure 2
【課題】アバタ、スワール等の外観不良が抑制された発泡成形体、成形体の外観不良を抑制することが可能な発泡成形体の製造方法、及び発泡成形体の外観不良の抑制方法を提供する。【解決手段】発泡層と、前記発泡層を被覆するスキン層と、を備え、前記発泡層における気泡の最大径が0.50mm以下であり、前記発泡層における、前記気泡の最大径と同一断面で測定される気泡の平均径が0.05mm~0.15mmであり、前記最大径及び前記平均径を有する前記気泡は発泡剤の熱分解により形成される気泡である、発泡成形体;及び、発泡成形体の製造方法又は外観不良の抑制方法。【選択図】図2 |
Author | MITSUISHI NAOKO HIRAI YOJI FUJINO HIROAKI SHIOKAWA HIROFUMI YAMADA KOJI NAKANO SHINGO |
Author_xml | – fullname: HIRAI YOJI – fullname: MITSUISHI NAOKO – fullname: FUJINO HIROAKI – fullname: NAKANO SHINGO – fullname: SHIOKAWA HIROFUMI – fullname: YAMADA KOJI |
BookMark | eNrjYmDJy89L5WRocvN39NX19fdxcXVRCAjydwl1DtFR8HUN8fB3UfB3U_B19At1c3QOCQ3y9HNXwKrY0c8FSUNwaEBAkGtwMEh5gL9_kIJjQICrY5Cjn7MrSBqLCTwMrGmJOcWpvFCam0HJzTXE2UM3tSA_PrW4IDE5NS-1JN4rwMjAyNjAwsDQ3NjRmChFALcoPpQ |
ContentType | Patent |
DBID | EVB |
DatabaseName | esp@cenet |
DatabaseTitleList | |
Database_xml | – sequence: 1 dbid: EVB name: esp@cenet url: http://worldwide.espacenet.com/singleLineSearch?locale=en_EP sourceTypes: Open Access Repository |
DeliveryMethod | fulltext_linktorsrc |
Discipline | Medicine Chemistry Sciences |
DocumentTitleAlternate | 発泡成形体、発泡成形体の製造方法、及び発泡成形体の外観不良の抑制方法 |
ExternalDocumentID | JP2023080173A |
GroupedDBID | EVB |
ID | FETCH-epo_espacenet_JP2023080173A3 |
IEDL.DBID | EVB |
IngestDate | Fri Sep 06 06:13:43 EDT 2024 |
IsOpenAccess | true |
IsPeerReviewed | false |
IsScholarly | false |
Language | English Japanese |
LinkModel | DirectLink |
MergedId | FETCHMERGED-epo_espacenet_JP2023080173A3 |
Notes | Application Number: JP20230062363 |
OpenAccessLink | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20230608&DB=EPODOC&CC=JP&NR=2023080173A |
ParticipantIDs | epo_espacenet_JP2023080173A |
PublicationCentury | 2000 |
PublicationDate | 20230608 |
PublicationDateYYYYMMDD | 2023-06-08 |
PublicationDate_xml | – month: 06 year: 2023 text: 20230608 day: 08 |
PublicationDecade | 2020 |
PublicationYear | 2023 |
RelatedCompanies | RESONAC HOLDINGS CORP |
RelatedCompanies_xml | – name: RESONAC HOLDINGS CORP |
Score | 3.6072965 |
Snippet | To provide a foam-molded product in which poor appearance such as pockmarks and swirls are suppressed, a method of manufacturing a foam-molded product capable... |
SourceID | epo |
SourceType | Open Access Repository |
SubjectTerms | AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING CHEMISTRY COMPOSITIONS BASED THEREON GENERAL PROCESSES OF COMPOUNDING METALLURGY ORGANIC MACROMOLECULAR COMPOUNDS PERFORMING OPERATIONS SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR SHAPING OR JOINING OF PLASTICS THEIR PREPARATION OR CHEMICAL WORKING-UP TRANSPORTING WORKING OF PLASTICS WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL WORKING-UP |
Title | FOAM-MOLDED PRODUCT, METHOD OF MANUFACTURING FOAM-MOLDED PRODUCT, AND METHOD OF SUPPRESSING POOR APPEARANCE OF FOAM-MOLDED PRODUCT |
URI | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20230608&DB=EPODOC&locale=&CC=JP&NR=2023080173A |
hasFullText | 1 |
inHoldings | 1 |
isFullTextHit | |
isPrint | |
link | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfV3NT8IwFH9BNOpNUaOipjFmJxeVFQaHxZS2CyFubXAz3Eg3IFETIDLj3b_ctoJyINzavvYlbfP6fm3fB8BNfaw0rshb7liTXez5Y1epYe6qoZePTLZtZcMuRnGjk-Juv94vwfvSF8bGCf2ywRG1ROVa3gt7Xs_-H7GYta2c32Wvumn6GCYBcxa3Y4On75sOawdcCiaoQ2nQlU7c-6Xp09j3yBZsGxxtAu3zl7ZxS5mt6pTwAHakZjcpDqH0piqwR5ep1yqwGy1-vHVxIXzzI_gOBYncSDwxzpDsCZbS5BZFPOkIhkSIIhKnIaFJagwc0NrOJGYrA55TaTfAdJdC9BCRkhNjuscNeQ2HY7gOeUI7rp7M4G_pBl25MnHvBMqT6WR0CqjRUPjBNynGsIe1RldZ08M1nGkAkbU0iDiD6gZG5xupVdg3NWtP1byAcvHxObrUmrvIruyK_wBx8JGH |
link.rule.ids | 230,309,786,891,25594,76906 |
linkProvider | European Patent Office |
linkToHtml | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfV3NT8IwFH9BNOJNUaPix2LMTi5-rDA4EFPaLRPp2uBmuJFuQKImQGTGu3-5bQXlQLg1_bUvaZvX92v7-h7AVXUkFa_IGs5IwQ5yvZEj5SBz5MDNhjrbtjRhF1lUCxPU7lV7BXhf_IUxcUK_THBEpVGZ0vfc7NfT_0ssanwrZzfpq6qaPARxk9rz07Hm07d1m7aavuCUE5uQZlvYUfcXU7ux5-IN2PR0eF7NnV5a-lvKdNmmBLuwJZS4cb4HhTdZhhJZpF4rwzabv3ir4lz5ZvvwHXDMHMY71KeW6HKakPjaYn4ccmrxwGI4SgJM4kQ7OFgrG-OILnV4ToRZAN1ccN61sBA-1q57voZXSDiAy8CPSeiowfT_pq7fFksDdw-hOJ6Mh0dg1WoS3Xk6xRhykbLoMq276B6likCkDUUijqGyRtDJWvQCSmHMOv3OY_RUgR2NGN-q-ikU84_P4Zmy4nl6bmb_B2nclHQ |
openUrl | ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Apatent&rft.title=FOAM-MOLDED+PRODUCT%2C+METHOD+OF+MANUFACTURING+FOAM-MOLDED+PRODUCT%2C+AND+METHOD+OF+SUPPRESSING+POOR+APPEARANCE+OF+FOAM-MOLDED+PRODUCT&rft.inventor=HIRAI+YOJI&rft.inventor=MITSUISHI+NAOKO&rft.inventor=FUJINO+HIROAKI&rft.inventor=NAKANO+SHINGO&rft.inventor=SHIOKAWA+HIROFUMI&rft.inventor=YAMADA+KOJI&rft.date=2023-06-08&rft.externalDBID=A&rft.externalDocID=JP2023080173A |