METHOD FOR PRODUCING MALEIMIDE RESIN
To provide a method for producing a maleimide resin, which can reduce a residual amount of solvent, enables synthesis in a short time, and can suppress side reactions during synthesis.SOLUTION: There is provided, a method for producing a maleimide resin obtained by reacting a tetracarboxylic acid di...
Saved in:
Main Authors | , |
---|---|
Format | Patent |
Language | English Japanese |
Published |
30.05.2023
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | To provide a method for producing a maleimide resin, which can reduce a residual amount of solvent, enables synthesis in a short time, and can suppress side reactions during synthesis.SOLUTION: There is provided, a method for producing a maleimide resin obtained by reacting a tetracarboxylic acid dianhydride (a1), a diamine (a2), and maleic anhydride (a3), comprising: a half-esterification step of mixing a (a1) component and a mixed solvent to half-esterify the (a1) component; an imidization step of adding a (a2) component to the half-esterified (a1) component to perform a dehydration cyclization reaction to obtain a polyimide resin; and a maleimidization step of adding a (a3) component to the polyimide resin to perform a dehydration cyclization reaction to obtain a maleimide resin, where the mixed solvent comprises an aromatic hydrocarbon having a boiling point of 150°C or higher and an alcohol having a boiling point of 100°C or lower and the (a2) component comprises a dimer diamine and a second diamine other than the dimer diamine.SELECTED DRAWING: None
【課題】溶媒の残留量を低減でき、短時間で合成が可能であり、合成時の副反応を抑制可能なマレイミド樹脂の製造方法の提供。【解決手段】テトラカルボン酸二無水物(a1)、ジアミン(a2)、及び無水マレイン酸(a3)を反応させてなるマレイミド樹脂の製造方法であって、(a1)成分と混合溶媒とを混合して(a1)成分をハーフエステル化するハーフエステル化工程と、ハーフエステル化した(a1)成分に(a2)成分を添加して脱水閉環反応を行い、ポリイミド樹脂を得るイミド化工程と、ポリイミド樹脂に(a3)成分を添加して脱水閉環反応を行い、マレイミド樹脂を得るマレイミド化工程と、を有し、混合溶媒が、沸点150℃以上の芳香族炭化水素と沸点100℃以下のアルコールとを含有し、(a2)成分が、ダイマージアミンとダイマージアミン以外の第2のジアミンとを含有する、製造方法。【選択図】なし |
---|---|
Bibliography: | Application Number: JP20220183496 |