RECYCLED POLYESTER RESIN AND METHOD FOR PRODUCING RECYCLED POLYESTER RESIN
To provide a copolyester resin using a recycled polyester raw material as a raw material.SOLUTION: There is provided a recycled polyester resin which is a polyester resin containing a component derived from a recycled polyester raw material and satisfies all of the following (1) to (4). (1) When a t...
Saved in:
Main Authors | , , |
---|---|
Format | Patent |
Language | English Japanese |
Published |
03.03.2023
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Abstract | To provide a copolyester resin using a recycled polyester raw material as a raw material.SOLUTION: There is provided a recycled polyester resin which is a polyester resin containing a component derived from a recycled polyester raw material and satisfies all of the following (1) to (4). (1) When a total amount of all acid components constituting a polyester is defined as 100 mol%, a content of terephthalic acid is 50 to 98 mol% and a content of isophthalic acid is 2 to 50 mol%, (2) when a total amount of all glycol components is defined as 100 mol%, a content of ethylene glycol is 80 mol% or more and the content of diethylene glycol is 4 mol% or less, (3) carboxyl end group concentration is 40 equivalent/t or less and (4) an average pressure increase rate is 0.6 MPa/h or less.SELECTED DRAWING: None
【課題】リサイクルポリエステル原料を原料とする共重合ポリエステル樹脂を提供する。【解決手段】リサイクルポリエステル原料に由来する成分を含むポリエステル樹脂であって、下記の(1)~(4)を全て満足する再生ポリエステル樹脂。(1)ポリエステルを構成する全酸成分の合計量を100モル%とするとき、50~98モル%がテレフタル酸、2~50モル%がイソフタル酸であり、(2)全グリコール成分の合計量を100モル%とするとき、エチレングリコールが80モル%以上、ジエチレングリコールが4モル%以下であり、(3)カルボキシル末端基濃度が40当量/t以下であり、(4)平均昇圧速度が0.6MPa/h以下である再生ポリエステル樹脂。【選択図】なし |
---|---|
AbstractList | To provide a copolyester resin using a recycled polyester raw material as a raw material.SOLUTION: There is provided a recycled polyester resin which is a polyester resin containing a component derived from a recycled polyester raw material and satisfies all of the following (1) to (4). (1) When a total amount of all acid components constituting a polyester is defined as 100 mol%, a content of terephthalic acid is 50 to 98 mol% and a content of isophthalic acid is 2 to 50 mol%, (2) when a total amount of all glycol components is defined as 100 mol%, a content of ethylene glycol is 80 mol% or more and the content of diethylene glycol is 4 mol% or less, (3) carboxyl end group concentration is 40 equivalent/t or less and (4) an average pressure increase rate is 0.6 MPa/h or less.SELECTED DRAWING: None
【課題】リサイクルポリエステル原料を原料とする共重合ポリエステル樹脂を提供する。【解決手段】リサイクルポリエステル原料に由来する成分を含むポリエステル樹脂であって、下記の(1)~(4)を全て満足する再生ポリエステル樹脂。(1)ポリエステルを構成する全酸成分の合計量を100モル%とするとき、50~98モル%がテレフタル酸、2~50モル%がイソフタル酸であり、(2)全グリコール成分の合計量を100モル%とするとき、エチレングリコールが80モル%以上、ジエチレングリコールが4モル%以下であり、(3)カルボキシル末端基濃度が40当量/t以下であり、(4)平均昇圧速度が0.6MPa/h以下である再生ポリエステル樹脂。【選択図】なし |
Author | TOMIMORI YASUHIRO ONO KATSUNORI TEMMAN YUTA |
Author_xml | – fullname: ONO KATSUNORI – fullname: TEMMAN YUTA – fullname: TOMIMORI YASUHIRO |
BookMark | eNrjYmDJy89L5WTwCnJ1jnT2cXVRCPD3iXQNDnENUghyDfb0U3D0c1HwdQ3x8HdRcPMPUggI8ncJdfb0c1fApYOHgTUtMac4lRdKczMoubmGOHvophbkx6cWFyQmp-allsR7BRgZGBkbGFkYmBo7GhOlCAD6mi_B |
ContentType | Patent |
DBID | EVB |
DatabaseName | esp@cenet |
DatabaseTitleList | |
Database_xml | – sequence: 1 dbid: EVB name: esp@cenet url: http://worldwide.espacenet.com/singleLineSearch?locale=en_EP sourceTypes: Open Access Repository |
DeliveryMethod | fulltext_linktorsrc |
Discipline | Medicine Chemistry Sciences |
DocumentTitleAlternate | 再生ポリエステル樹脂及び再生ポリエステル樹脂の製造方法 |
ExternalDocumentID | JP2023028053A |
GroupedDBID | EVB |
ID | FETCH-epo_espacenet_JP2023028053A3 |
IEDL.DBID | EVB |
IngestDate | Fri Jul 19 12:46:03 EDT 2024 |
IsOpenAccess | true |
IsPeerReviewed | false |
IsScholarly | false |
Language | English Japanese |
LinkModel | DirectLink |
MergedId | FETCHMERGED-epo_espacenet_JP2023028053A3 |
Notes | Application Number: JP20210133504 |
OpenAccessLink | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20230303&DB=EPODOC&CC=JP&NR=2023028053A |
ParticipantIDs | epo_espacenet_JP2023028053A |
PublicationCentury | 2000 |
PublicationDate | 20230303 |
PublicationDateYYYYMMDD | 2023-03-03 |
PublicationDate_xml | – month: 03 year: 2023 text: 20230303 day: 03 |
PublicationDecade | 2020 |
PublicationYear | 2023 |
RelatedCompanies | UNITIKA LTD NIPPON ESTER CO LTD UNITIKA TRADING CO LTD |
RelatedCompanies_xml | – name: UNITIKA LTD – name: NIPPON ESTER CO LTD – name: UNITIKA TRADING CO LTD |
Score | 3.5893636 |
Snippet | To provide a copolyester resin using a recycled polyester raw material as a raw material.SOLUTION: There is provided a recycled polyester resin which is a... |
SourceID | epo |
SourceType | Open Access Repository |
SubjectTerms | APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS CHEMISTRY COMPOSITIONS BASED THEREON MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS METALLURGY NATURAL OR ARTIFICIAL THREADS OR FIBRES ORGANIC MACROMOLECULAR COMPOUNDS SPINNING TEXTILES THEIR PREPARATION OR CHEMICAL WORKING-UP |
Title | RECYCLED POLYESTER RESIN AND METHOD FOR PRODUCING RECYCLED POLYESTER RESIN |
URI | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20230303&DB=EPODOC&locale=&CC=JP&NR=2023028053A |
hasFullText | 1 |
inHoldings | 1 |
isFullTextHit | |
isPrint | |
link | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfR1dT8Iw8IJo1DdFjYqaxpi9LeK-kAdioO0cC_sIDgNPZJ0lUZNBZMa_762C8iLpy7VNm_ba6921d1eAGyHthtNyprqDlKQjh5a6sC1Dl2aW4nJnmaEchYPQ8YaWP7JHFXhf-cKoOKFfKjgiUlSG9F6o83r-d4nFlG3l4la8YtHswU3aTFtqxyhPY9JYt83jiEVUo7Ttx1o4-Kkz7nHLdbZgu5Sjy0D7_LlbuqXM13mKewA7MXaXF4dQeUtrsEdXX6_VYDdYvngjuCS-xRH4A07HtM8ZiaP-mD-hIEoQf72QdEJGAp54ESOo1JF4ELEh7YWP5L8Wx3Dt8oR6Og5q8ouCiR-vTcA8gWo-y-UpkFbzzmiKFOUmKayplaYSOXDmIGjazRezcQb1DR2db6ytw36ZUwZX5gVUi49PeYkcuBBXCnPfUwSCtQ |
link.rule.ids | 230,309,786,891,25594,76906 |
linkProvider | European Patent Office |
linkToHtml | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfR1dT8Iw8IJoxDdFDYofjTF7W8R9ysNioB1uc1_BYeCJbLMkagJEZvz73iooL5K-NL300l57vbv27gpwnXG9ZbSNiWwgJ8koobmc6ZoiczVPcbnzXBGBwkFoOAPNG-rDCryvYmFEntAvkRwROSpHfi_EeT3_u8RiwrdycZO9YtPsvpdYTFpax6hPY5FY17LjiEVUotTyYins_8CUO9xynS3YNsv0vKXu9Nwtw1Lm6zKltw87MaKbFgdQeUvrUKOrr9fqsBssX7yxumS-xSF4fZuOqG8zEkf-yH5CRZQg_dyQdEJGAjtxIkbQqCNxP2ID6oYP5L8eR3DVsxPqyDio8S8Jxl68NgH1GKrT2ZQ3gLTNW8XMUtSbeKZNtDTlKIFzA6uqbr6orRNobkB0uhF6CTUnCfyx74aPTdgrIcL5Sj2DavHxyc9RGhfZhaDiN5jBhaI |
openUrl | ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Apatent&rft.title=RECYCLED+POLYESTER+RESIN+AND+METHOD+FOR+PRODUCING+RECYCLED+POLYESTER+RESIN&rft.inventor=ONO+KATSUNORI&rft.inventor=TEMMAN+YUTA&rft.inventor=TOMIMORI+YASUHIRO&rft.date=2023-03-03&rft.externalDBID=A&rft.externalDocID=JP2023028053A |