Cover

Loading…
More Information
Summary:PROBLEM TO BE SOLVED: To provide a method for forming a lithium thin film with which a lithium thin film with high purity can be always produced so as to improve service capacity of lithium. SOLUTION: A lithium or lithium alloy material is heated and evaporated to produce ultrafine particles of the lithium or lithium alloy within a ultrafine particle production chamber in an inert gas atmosphere having purity of ≥99.9995%. The ultrafine particles are carried into a film formation chamber in a vacuum atmosphere by a carrier tube while being accompanied with the inert gas. The ultrafine particles are injected under the pressure of the inert gas from a nozzle fitted to the tip of the carrier tube and heated to the melting point of the ultrafine particle or below toward a substrate arranged in the film formation chamber. Further, either the nozzle or the substrate is moved at an optional moving speed, thus a lithium or lithium alloy thin film is formed on the substrate. Before the inert gas is introduced into the vacuum chamber, the ultimate vacuum in the film formation chamber by an evacuation system is controlled to ≤5×10-4Pa. COPYRIGHT: (C)2007,JPO&INPIT
Bibliography:Application Number: JP20050250687